Metal melting propane furnace construction
<b>I just had one of those once-a-year ideas.</b>
Imagine dental casting cement (phosphate bonded cement). It's retains most of its strength when dehydrated and the shrinkage is only about 0.5%
-- and it's good for casting gold, which means it can easily handle a propane flame.
Then image mixing it with perlite (a volcanic mineral made up of mostly air), the second-to-none-except-vermiculite-or vaccuum insulator.
Guess who's going to buy a 25kg sack of phosphate bonded cement tomorrow?
I'll use this thread for documenting my new furnace construction process.
[Edited on 5-12-2004 by Polverone]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
Marvin
National Hazard
  
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
According to a random webpage, expanded perlite softens at 871-1093°C.
Introducing closed pore minerals or air bubbles into the cement sounds like a good way to make your kiln explode when you fire it.
Whats wrong with ordinary firebrick?
|
|
|
Hermes_Trismegistus
National Hazard
  
Posts: 602
Registered: 27-11-2003
Location: Greece, Ancient
Member Is Offline
Mood: conformation:ga
|
|
| Quote: | Originally posted by Marvin
According to a random webpage, expanded perlite softens at 871-1093°C.
|
Pearlite seems like a good choice, I'm sure the phosphate cement matrix will hold the soft beads in place and they'll reharden.
As for the vermiculite, I don't know about the insulation properties of the stuff, but it'll absorb water like nobody's business..
In masonry walls pearlite was used, cheap like borsht and repelled water like the anus of a duck.
Arguing on the internet is like running in the special olympics; even if you win: you\'re still retarded.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Explode!?
| Quote: |
Introducing closed pore minerals or air bubbles into the cement sounds like a good way to make your kiln explode when you fire it.
|
That's funny, my previous furnace has been operated for months without exploding.... besides, the cement is permeable to gasses when dehydrated.
It's used for casting jewelry and dental pieces.
Ooooooooh..... I really should get a car.... I just carried a 23kg floppy sack of phosphate bonded cement home..... my back.... my arms.... and wait!
I haven't eaten today! Perhaps I should do that.
Edit1: Then it's off to IKEA to buy that lidded bucket thingy.... I feel like I'm going to faint.
Edit2: | Quote: |
Whats wrong with ordinary firebrick?
|
Nothing, but I want a circular furnace intersection. Btw, some firebricks actually contain perlite, I read it somewhere yesterday.
[Edited on 2004-5-6 by axehandle]
[Edited on 2004-5-6 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
4s2
Harmless
Posts: 34
Registered: 9-4-2004
Location: Iowa US
Member Is Offline
Mood: Inspired
|
|
What does your old furnace look like? If you use brick I assume you just stacked bricks into a box. If so, what did you use to insulate the joints?
I built a cheapo box for $12 from the brick shop, and surrounded it on all sides with quarter inch steel plate. I was contemplating making a new one
that would heat better. This sounds interesting. keep us updated.
I haven\'t failed, I\'ve found 683 ways that don\'t work. -- Me.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
My old furnace
It looked like this:

The outer shell is a mild steel waste bin. The refractory was a mix I developed myself incorporating ideas from many others. Basically it's
fireproof cement, bentonite and perlite. The burner is stuck in through a tangentially aligned steel pipe at the bottom of the inside hollow cylinder.
The new one will use almost the same design, but it will be equipped with a hinged lid, it will be larger (much larger), and I will use a different
refractory composition. I'm going to use this investment cement: http://www.srs-ltd.co.uk/invest.html
together with perlite, the perlite being packed together maximally. Mostly air, so to speak.
I'll use the same home-built burner, it's documented here: http://species8472.dyndns.org/burner/burner.html
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
rikkitikkitavi
Hazard to Others
 
Posts: 192
Registered: 17-6-2002
Member Is Offline
Mood: No Mood
|
|
what is wrong with the present refractory?
perlite + fire proof cement which itself could withstand atleast 1200 C?
/rickard
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
| Quote: |
what is wrong with the present refractory?
perlite + fire proof cement which itself could withstand atleast 1200 C?
|
It takes a week to cure and dry, and is expensive (fire proof cement is actually quite expensive in large quantities). Also, it develops cracks after
months of (ab)use. Finally, it's a horrible mess to blend by hand.
The new refractory will only need 90 minutes to cure, and then it just has to be dehydrated. And I believe it can withstand temperatures up to 2000C,
someone told me something about casting platinum using it (as a mold).
Edit: NO, i stand corrected. It can only take 1400 or so... but that's enough for my purposes.
Edit2: To give you all an impression of the size of the soon-to-be furnace (I'm right now experimenting with mixing the cement with water-soaked
perlite), I present this picture. I am about 1.75m tall and quite sturdy, weighing in at about 82kg. It sure is one big bucket!

[Edited on 2004-5-6 by axehandle]
[Edited on 2004-5-6 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Vibrator.
To cast this, I'll need a vibrator that can shake the bucket when it weighs about 30kg. Any ideas? I'm in need of some help, my creativeness
quota for today is exceeded....
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
BromicAcid
International Hazard
   
Posts: 3320
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Take a large motor and put something on the turn shaft that is unevenly weighted, it will vibrate at high speed, experiment with different speeds and
weight dispersions for the best results. Heavily wound tape works well for fine tuning.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
| Quote: |
Take a large motor and put something on the turn shaft that is unevenly weighted, it will vibrate at high speed, experiment with different speeds and
weight dispersions for the best results. Heavily wound tape works well for fine tuning.
|
Thank you. That will be easy.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Some success.
The hard thing is finding the right water ratio, since soaked perlite oversaturates the cement mix with water. But I think I'm on the right track
with batch #5:

Edit: I'm off for the weekend now. No updates until Monday...
[Edited on 2004-5-7 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
OK, conclusions.
1) The dehydrated mix of phosphate cement and perlite was the best refractory material I've ever held in my hand. A block 15mm thick could be put
on a 2500W hotplate at full blast for 40 minutes and still feel only lukewarm at it's top.
2) The same material breaks when a fly lands on it, or when the tide shifts.
Conclusion: It can only be used if protected by a layer of another material preserving its structural integrity. Such as, e.g., a fireclay chimney
pipe in a metal bucket, refractory cast into the "outer shell".
But I'm not going to bother. I'll use the standard: Portland cement, bentonite, perlite and water. Perhaps a little bit of sand as well.
Lesson learned: Bright ideas are often not.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
OK
The last needed part for the new furnace is in my hands: A 15 litre thin, tall bucket (actually a plastic trashbin) to be used as the inside mold.
Expect a Sturmangriff of pictures tonight.
Step 1) Here is the bentonite, mixed with water. Actually it's a water suspension of kitty litter (mostly bentonite). It looks like someone has
had a severe case of some stomach illness....

Step 2) The outer shell and its lid. Here is a panorama image of the bucket with its now hinged lid:

And here is a closeup of the lid. Those 18 angle irons will hold the lids refractory block in place. To cast it, I'll simply surround the circle
of irons with a plastic strip and pour (with the lid horisontal, upside down). There's already a PP pipe in the middle to form the top vent.

Another closeup of the lid, hinges temporarily removed so I can cast the refractory for both furnace and lid simultaneously:

Here it is, the whole bucket with its lid closed:

I have to take a break now, my back is hurting like hell (yes, I have a very bad back).
[Edited on 2004-5-12 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Phew!
All done. But a word of advise: don't mix concrete by hand:

This is really gonna hurt tomorrow....
Edit: It's dripping pus and blood.... seems I got a really nasty alkaline burn from the calcium hydroxide in the cement....
[Edited on 2004-5-13 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
Magpie
lab constructor
   
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
caustic burns
Your total dedication to your projects is astounding! You have replaced vulture as my idol.
But seriously, I'm sorry to hear of your caustic burns. Take good care to allow healing as well as possible.
When a young man I was helping to poor a concrete slab. I was wearing rubber boots but the wet concrete worked its way in between my legs, just below
the knees (in front), and the boots. As a result of the abrasion/caustic I had permanent scars that didn't disappear for decades.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
Thank you. BromicAcid suggested vinegar, but since I didn't have any I mixed a VERY dilute HCl (aq) solution and dipped my hands in that. That,
followed by thorough cleaning and applying an acidic hand lotion have helped, it seems. The pus has almost stopped coming and it doesn't hurt as
much anymore.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
4s2
Harmless
Posts: 34
Registered: 9-4-2004
Location: Iowa US
Member Is Offline
Mood: Inspired
|
|
while working on with my quest to find out more and more about thermit welding... I found out that the crucibles used to withstand the heat of the
reactions of Fe3O4+Al (apparently this combination burns at 3 times the temp that Fe203+Al burns at) used Magnesite(MgCO3). (shelled by regular steel)
I also read in an old Metallurgy book from 1914, that dolomite (MgCa(CO3)2) was used in furnaces to retain heat required to smelt steel.
My geology friend(GF) says that neither is especialy difficult to find/extract if you know what to look for, however you may need to find a way to
bind the dolomite particles together) I dont know why I didnt ask my GF this before about refractory materials... duh.
I haven\'t failed, I\'ve found 683 ways that don\'t work. -- Me.
|
|
|
4s2
Harmless
Posts: 34
Registered: 9-4-2004
Location: Iowa US
Member Is Offline
Mood: Inspired
|
|
bucket of doom
on another note... What is that bucket made out of? rather... thats not galvanized is it?
I haven\'t failed, I\'ve found 683 ways that don\'t work. -- Me.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
It's galvanized alright... but the heat will never be in contact with the galv. steel, there's refractory between them ---- I know about the
toxic fumes.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
4s2
Harmless
Posts: 34
Registered: 9-4-2004
Location: Iowa US
Member Is Offline
Mood: Inspired
|
|
heh thats what I said about my 2nd furnace. Zinc Oxide would fume off the sides over a long period of time.
What do you think about using Magnesite? I will try to do this *adds another project to his warboard*
I haven\'t failed, I\'ve found 683 ways that don\'t work. -- Me.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
My old furnace was galvanized too. No zinc oxide there.... my refractory is pretty good.
I'm wondering how dangerous it really is, after all it's used in white paint. It's probably the risk of silicosis that's the
danger, which could be averted by wearing breating protection...
Or, one could simply sand off the zinc, or remove it with HCl.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
Organikum
resurrected
   
Posts: 2344
Registered: 12-10-2002
Location: Europe
Member Is Offline
Mood: frustrated
|
|
Remove it with NaOH. This will take the zinc away but wont attack the iron so bad as HCl does. If you want to use HCl, use it in diluted form - 5% to
10%.
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
ho, ho, ho...
My hand looks as if it will be healed in about a week. I'm testing my (presumably failed) refractory mix now. There was a bit of a.... eeeehhh...
backdraft..... so I'll have to cut my beard a bit short. The fuel/air explosion took some of it away, which was annoying but not painful.
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
axehandle
Free Radical
   
Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline
Mood: horny
|
|
I'll be damned.
The new furnace seems to hold together. The refractory hasn't cracked yet (I'm drying it out at full blast). If only I knew what the evil
fumes coming from it are. They irritate my eyes but don't seem to affect the lungs. It's probably water and perlite dust, perhaps with some
ZnO added in for comic relief....
We'll see, I'm beginning to feel hope again...
Please note that I wouldn't advice anyone to repeat my experiment. My lungs are my own, I'm only risking my own health here.
If the whole thing works, I'll get a propane refill tomorrow or the next day, then it's FINALLY casting time. If I could only find a decent
crucible (i.e. cast iron, not thinwalled stainless)....
Edit: Out of propane. The refractory seems fine. I'll have to let it cool down slowly, the propane didn't last long enough for all those
pesky water moleculles to be driven out. More to come.
On crucibles, I have a request for comments. You see, I have this old 80mm ID, 90mm OD cast iron old sewage pipe which I found at a construction site.
What if I cut off a piece, say 250mm long, and construct this:

It should work, but I feel I've missed something really obvious?
[Edited on 2004-5-24 by axehandle]
My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35
\"Verbing nouns weirds the language!\"
|
|
|
| Pages:
1
2
3 |