Search |
[Next Page] |
Hydrogen Peroxide Production hi,
i have various information about H2O2 Production but these patent has no instruction for making ... |
24-8-2008 at 00:48 by: Fashist |
Trinitrotoluene preparation [quote][i]Originally posted by CD-ROM-LAUFWERK[/i]
my TNT did melt around 81°C, wich is pure
the ... |
15-3-2008 at 05:05 by: Fashist |
Trinitrotoluene preparation Its true.
Merck Trifluoromethanesulfonic acid is 56 eur per liter. |
1-3-2008 at 01:26 by: Fashist |
Trinitrotoluene preparation I Found Interesting Patent
http://www.freepatentsonline.com/WO2005005342.html
Nitric Acid+Trifluor ... |
1-3-2008 at 01:01 by: Fashist |
Acetic anhydride preparation Merck SICL4 is 56$ per liter(cheap than Alfa)
If you order drum(190kg) it will be cheaper. |
29-2-2008 at 00:50 by: Fashist |
starch Problem! Mr spark i didnt find that here(no chmical strore dont know what is that) |
24-2-2008 at 13:49 by: Fashist |
starch Problem! thanks mr not important
gluco-amylase seems be better.
anybody know company that sale it?
thx
[E ... |
24-2-2008 at 11:34 by: Fashist |
starch Problem! spit into my starch?
sure i search it before and i didnt find. |
24-2-2008 at 07:09 by: Fashist |
starch Problem! Thanks of you
Mr sauron tapioca is commonly plant?(may i find that?)
Mr evil gluco-amylase is comm ... |
24-2-2008 at 06:48 by: Fashist |
starch Problem! Thanks
I search it before but most of patent use plant like Cassava and koji kom and.. for hydrolyz ... |
24-2-2008 at 03:45 by: Fashist |
starch Problem! i am looking for cheap component that broke starch to glucose
thx |
24-2-2008 at 01:45 by: Fashist |
Acetic anhydride preparation Today i test the pyrosulphate method but no result!
i mix 250gram k2s2o7 and 165gram acona and add ... |
22-2-2008 at 13:57 by: Fashist |
Acetic anhydride preparation Mr sauron you think potassium pyrosulphate wont work?
K2S207+ACONA->AC2O+na2so4+k2so4?
or
NA2S ... |
20-2-2008 at 01:24 by: Fashist |
Acetic anhydride preparation I will try
K2S207+ACONA->AC2O+na2so4+k2so4
i just find pottasium pyrosulphate(old merck product ... |
19-2-2008 at 04:41 by: Fashist |
Acetic anhydride preparation Now i cant Product any acetic anhydrid because merck dont sale acetyle chloride.(germany cut its tra ... |
19-2-2008 at 03:56 by: Fashist |
Acetic anhydride preparation i think this is not good method because pocl3 is very toxic.
anybody has experience with sodium pyr ... |
18-2-2008 at 23:23 by: Fashist |
Acetic anhydride preparation 6 PCl5 + P4O10 → 10 POCl3
"Phosphorus pentachloride also forms POCl3 by reaction with w ... |
17-2-2008 at 20:55 by: Fashist |
Acetic anhydride preparation POCL3+4ACONA->2AC2O+3NACL+NAPO3
Good idea
any body has idea? |
17-2-2008 at 10:22 by: Fashist |
Trinitrotoluene preparation My Suggestion is Using Con.Nitric Acid
I Made it Using Dry Mg(NO3)2 + HNO3(57%) and then Distil. |
10-2-2008 at 12:03 by: Fashist |
Trinitrotoluene preparation I used this book Ratio
http://rapidshare.com/files/90231545/fmx.zip.html |
8-2-2008 at 12:31 by: Fashist |
Trinitrotoluene preparation I made tnt very easy by reflux system(see below picture)
First i made Dnt and then made tnt in the ... |
7-2-2008 at 22:46 by: Fashist |
Method For Drying Mg(No3)2 I made Mg(no3)2 before(MGCO3+HNO3).
I made nitric acid from an+h2so4 before but i want to try this ... |
1-2-2008 at 01:12 by: Fashist |
Method For Drying Mg(No3)2 Any body Know Simple Method For Drying Mg(No3)2 ?
and Anybody know how we can increase the concentr ... |
30-1-2008 at 03:48 by: Fashist |
keten lamp Mr Nicodem Soon I will Send Picture of My System.
You Said I Use .5 ml for Testing? |
21-1-2008 at 09:30 by: Fashist |
keten lamp My System is Larger than Normal System and I Need to Use 50cc Aniline Per Test.
My Acetone Boiler i ... |
19-1-2008 at 03:28 by: Fashist |