Broken tap remover active ingredients
Hello,
I am wondering what is in this stuff.
http://cgi.ebay.co.uk/Broken-tap-remover-Emergency-work-reco...
Dann2
|
|
|
Eclectic
National Hazard
  
Posts: 899
Registered: 14-11-2004
Member Is Offline
Mood: Obsessive
|
|
I don't know about that particular compound, but ammonium or sodium persulfate would work on aluminum, you might want to use just alum, sodium
bisulfate, or sulfuric acid on brass or copper. The persulfates would etch copper and brass, sulfuric acid and sodium bisulfate would probably attack
brass.
|
|
|
12AX7
Post Harlot
   
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
One remedy I heard was boiling in alum. Apparently it's acidic enough. Another is nitric or sulfuric acid, which obviously work best on aluminum.
Sulfuric, or, yeah, a bisulfate, is the best bet here.
Tim
|
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
sulfamic acid would be my guess
|
|
|