Alum Shale
I went on holiday to Sweden last year with my girlfriend and whilst we were there we went to a sort of nature place, like trees, streams, waterfalls.
But it was once an alum shale mine/quarry, and I found a infomation board that had (really vague) ingructions on how the alum was extracted and I
thought I'd give it a go, so I brought some home with me to give it a go. However, there isn't much on the internet about alum shale apart from a
short wiki page. So I was wondering if anyone knows anything about it that could help me with my extraction.
(Also, I'm going to document my attempt(s) on Youtube, so if you're interested, heres a link: My Channel)
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Does this help?
http://www.wovepaper.co.uk/alumessay2.html
|
|
|
Smooth203
Harmless
Posts: 21
Registered: 29-10-2016
Location: Lancaster - UK
Member Is Offline
Mood: No Mood
|
|
wow, that's perfect, thanks! I bet you found it so easily Unless of course you
already knew about it
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I googled "alum shale production"
it's the 4th hit.
|
|
|
Smooth203
Harmless
Posts: 21
Registered: 29-10-2016
Location: Lancaster - UK
Member Is Offline
Mood: No Mood
|
|
god damn, I'm so bad at finding stuff, thanks anyway!
|
|
|