Tantalum Recovery Experiment from Tantalum Capacitors


Part 1: https://www.youtube.com/watch?v=azN04e7_QWg
Part 2: https://www.youtube.com/watch?v=y6x8fB9k10Y
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 30-12-2016 at 07:11


Could you please post some text, information, discussion when posting your videos? Because otherwise it's just outright ummm promotion of your stuff, especially since you are posting them in separate threads.

Side note: selenium might have been oxidised by air partially in your other video, but should be fine. Should you have some metal powders, you could try to synthesise some selenides too, it should be fun.





there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
diddi
National Hazard
****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 30-12-2016 at 11:22


^
easily mistaken for spam




Beginning construction of periodic table display
View user's profile View All Posts By User

  Go To Top