I've read that this can be done by heating it, but how much heat does it take? Would charcoal + lots of air do it or would it take a high current carbon-arc type setup?
View user's profile View All Posts By User
madscientist
National Hazard
****




Posts: 962
Registered: 19-5-2002
Location: American Midwest
Member Is Offline

Mood: pyrophoric

[*] posted on 18-5-2003 at 13:17


I once attempted to reduce MgSO<sub>4</sub> with charcoal (both powders, intimately mixed) in a charcoal fire. Nothing much seemed to happen.

[Edited on 18-5-2003 by madscientist]




I weep at the sight of flaming acetic anhydride.
View user's profile View All Posts By User
Theoretic
National Hazard
****




Posts: 776
Registered: 17-6-2003
Location: London, the Land of Sun, Summer and Snow
Member Is Offline

Mood: eating the souls of dust mites

[*] posted on 30-6-2003 at 04:24
Thermite?


Theoretically, Al powder would react with CaSO4 quite exothermically. SO4-- is more oxidizing than S.
View user's profile View All Posts By User
rikkitikkitavi
Hazard to Others
***




Posts: 192
Registered: 17-6-2002
Member Is Offline

Mood: No Mood

[*] posted on 1-7-2003 at 05:53


CaSO4 can be reduced with C , but it takes about 13-1400 C, wich is unobtainable in a simple charcoal fire, unless it is very large. Heat loss compared to combustion rate is unfavourable in most fires that we can construct in the lab or in a garden.

An arc oven (with graphite electrodes ) would probably work.