Pentaerythrite-Pentaerythritol 99% Source
http://www.ebay.com/itm/321747873140
..I have seached for years and finally found a reliable source
|
|
NeonPulse
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 417
Registered: 29-6-2013
Location: The other end of the internet.
Member Is Offline
Mood: Isolated from Reality! For Real this time....
|
|
Buying 1.7 kg of pentaerythritol wouldn't be the greatest idea since it's got very little uses outside of industry like paints and resins and
obviously explosives. Depending which country you live in you would likely have your door kicked in at 5am raided and arrested by homeland security.
|
|
BobD1001
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 182
Registered: 29-3-2013
Member Is Offline
Mood: No Mood
|
|
Well it looks like he sells smaller quantities as well. I purchased 150g mostly out of curiosity. Does anyone have any good non-pyro related uses for
it? I am mostly interested in its uses in resins and polymers.
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by BobD1001 ![](images/xpblue/lastpost.gif) | Well it looks like he sells smaller quantities as well. I purchased 150g mostly out of curiosity. Does anyone have any good non-pyro related uses for
it? I am mostly interested in its uses in resins and polymers. |
Maybe try heating with oxalic acid or urea to make a thermohardening resin...
C(-CH2-OH)4 + HO2C-CO2H -heat-> 3D-PE oxalate ester + H2O(g)
C(-CH2-OH)4 + H2N-CO-NH2 -heat-> 3D-PE carbonate ester + NH3(g)
May also work with terephtalic acid from PET bottles.
C(-CH2-OH)4 + HO2C-C6H4-CO2H -heat-> 3D-PE terephtalate ester + H2O(g)
[Edited on 11-6-2016 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Bert
|
Thread Moved 11-6-2016 at 19:35 |
BobD1001
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 182
Registered: 29-3-2013
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by PHILOU Zrealone ![](images/xpblue/lastpost.gif) |
Maybe try heating with oxalic acid or urea to make a thermohardening resin...
C(-CH2-OH)4 + HO2C-CO2H -heat-> 3D-PE oxalate ester + H2O(g)
C(-CH2-OH)4 + H2N-CO-NH2 -heat-> 3D-PE carbonate ester + NH3(g)
May also work with terephtalic acid from PET bottles.
C(-CH2-OH)4 + HO2C-C6H4-CO2H -heat-> 3D-PE terephtalate ester + H2O(g)
[Edited on 11-6-2016 by PHILOU Zrealone] |
Great suggestions, thank you! I'm hoping to learn some polymer chemistry, since I regrettably never to organic chem while I was in college.
|
|