Author: Subject: Question on this neat crystallization
Fidelmios
Hazard to Others
***




Posts: 104
Registered: 28-4-2016
Location: Witty Chemistry Joke
Member Is Offline

Mood: No Mood

[*] posted on 18-5-2016 at 23:58
Question on this neat crystallization


Hello all,
So I've began to dabble in Crystal growing, and I was curious about Double Salts. So I've got Ferrous Sulfate, and Copper Sulfate, and I decided to try and crystallize them. So I just threw two saturated solutions together and mix them. The result is what is show on the right, compared to Ferrous sulfate (left). http://imgur.com/AlmDEaP

It seems to maintain the crystal shape of Copper Sulfate, but with the color of a mixture of the two. Did I end up making a double salt, or something like it? Will they make one if I use proper equimolar equivalents?

On a side note, whenever I look at people's Ferrous Sulfate crystals they are near teal, mine are a light green. Why?
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3721
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 19-5-2016 at 02:10


I think that you have crystalised your solutions too quickly,
all show signs of agglomeration ....
some of the solution and its contents get trapped in the mass of crystals.
Hence the colour is not 'pure'.

For purity and aesthetics a single crystal is required,
if pure it will be transparent I believe.
View user's profile View All Posts By User
Fidelmios
Hazard to Others
***




Posts: 104
Registered: 28-4-2016
Location: Witty Chemistry Joke
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2016 at 10:28


The camera does not do this mass justice. The Ferrous Sulfate ones on the left are almost transparent. They have some minor discoloration due to the oxide layer being deposited on them.
View user's profile Visit user's homepage View All Posts By User
Hegi
Hazard to Others
***




Posts: 199
Registered: 27-9-2013
Member Is Offline

Mood: No idea.

[*] posted on 19-5-2016 at 11:15


As long as I know there is no double salt with structure of alternating Fe(II)/Cu(II) ions. :o



Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4355
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 19-5-2016 at 11:36


I believe you cannot get a double salt unless the ions are significantly different, so that they occupy different locations in the crystal structure. Otherwise you just get a mixed crystal.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Fidelmios
Hazard to Others
***




Posts: 104
Registered: 28-4-2016
Location: Witty Chemistry Joke
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2016 at 14:41


That was my question, it doesn't look like a double salt, so idk what I made.
View user's profile Visit user's homepage View All Posts By User
Xenoid
National Hazard
****




Posts: 775
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline

Mood: Comfortably Numb

[*] posted on 19-5-2016 at 15:05


From Mellor......

"It is interesting to note that copper sulphate normally crystallizes with 5H2O, but a salt isomorphous with the above series (Fe, Be,Mg, Zn, Cd, Mn, Cr, Co, Ni sulphates - the vitriols) and of the composition CuSO4.7H2O is formed when copper sulphate in admixture with the sulphate of Fe, Zn or Mg is allowed to crystallize."
View user's profile View All Posts By User
Hegi
Hazard to Others
***




Posts: 199
Registered: 27-9-2013
Member Is Offline

Mood: No idea.

[*] posted on 20-5-2016 at 10:16


Actually, I was wrong. There exist a compound naturally found as a mineral PISANITE with a composition of (Fe<sub>0.8</sub>Cu<sub>0.2</sub>;)SO<sub>4</sub>.7H<sub>2</sub>O. The ratio Cu/Fe of found specimens is fixed 1:5. There was also found ferrous sulfate heptahydrate (mellanterite) crystallizing as an overgrowth on pisanite.



Our webpage has been shut down forever cause nobody was willing to contribute. Shame on you all!!!
View user's profile View All Posts By User
Fidelmios
Hazard to Others
***




Posts: 104
Registered: 28-4-2016
Location: Witty Chemistry Joke
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2016 at 23:23


Neat! That is very interesting thank you Hegi
View user's profile Visit user's homepage View All Posts By User