[*] posted on 23-4-2016 at 02:10
new insulation for a heating mantle - aus


I was a bit divided on where to post this -- bad days in the lab, short questions... Decided on a new thread.

I had a nice little boil over distilling some nitric acid today and spilled hot saturated KHSO4 solution all over my mantle. It shorted to earth and flipped the circuit-breaker.

Pulling it apart the glass wool insulation was quite damp and seemed to be what was causing the shorting. I could dry and re-use it but there are couple of reasons for not doing that.
Firstly the glass fibres seem very short and brittle and not well interlocking -- the material is quite powdery and a pain to work with.
Secondly, I really should wash it thoroughly to remove any potassium bisulfate present. Otherwise I am going to get a melt when the element gets over 200C.

So I am looking for a suitable glass wool or felt to repack the mantle. I have not had a whole lot of success in finding pottery / kiln suppliers locally and have also had no success in the pizza oven area. I am assuming that standard house insulation is way below the grade needed. I had wondered about packing the space with fire-blanket material.

Can someone give me suggestions on a readily-available suitable insulation material?




View user's profile View All Posts By User
NedsHead
Hazard to Others
***




Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2016 at 02:37


Furnace builders use a ceramic wool called Kaowool, I've heard it is available in Aus but I don't know where from or how much it will cost, maybe rockwool can do the job? it's cheap and easily found at hydroponic shops
View user's profile View All Posts By User
Orenousername
Hazard to Self
**




Posts: 79
Registered: 16-4-2016
Location: USA
Member Is Offline

Mood: Regulated

[*] posted on 23-4-2016 at 04:48


I am unfamiliar with how the wiring in mantles is done, but if it thin, interlocking wires then i would suggest a carbon-clay mixture. A bit messy after a while but will hold up decently (does for my crucibles and shat together hot plate anyways)
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1638
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2016 at 04:56


rock wool I've usedon custom ovens befor and it seemed to do the job well.
View user's profile View All Posts By User
NedsHead
Hazard to Others
***




Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2016 at 05:15


with a heat resistance of 700-850c I think it'll do just fine https://en.wikipedia.org/wiki/Mineral_wool