What's the best way to recover Pd from Pd-Organic complexes?


I have a bunch of Pd that is bound to some organic (phosphine) complexes (in the form of PdCl2), and I want to recover the Pd for reuse.

I'm not sure if Aqua Regia will dissolve it. I thought maybe I could pyrolyze it first, but that may form Pd Oxides and I'm not sure if those will dissolve in aqua regia either.

Would it be as simple as heating the complex to a high enough temperature (300c+) to decompose/vaporize the organics, and siphon them off down the drain? I am not sure whether this will leave behind the Pd in salt form, or in metal/oxide form... I suspect if the temperature is kept low enough, the salt will remain in tact?
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 1-3-2016 at 17:46


Why not just recover the Pd(PPh3)2Cl2 as the complex? It's pretty useful itself. (I use it in my University research lab for Sonogashira couplings.)

Heating in an inert atmosphere would likely leave you with just palladium chloride. If you wanted palladium metal, you could electrolyze that.




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
FireLion3
Hazard to Others
***




Posts: 218
Registered: 11-1-2014
Member Is Offline

Mood: No Mood

[*] posted on 1-3-2016 at 18:04


I'll try heating it, though I don't think I have an inert atmosphere at my disposal, but metal salts don't usually oxidize at such low temperatures (under 350c), do they?

It's not just a palladium complex, but a mix of different complexes and polymeric material from faulty experiments - in other words, it's my Pd-waste container.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 1-3-2016 at 18:13


Heating in air is probably fine, but you could also try heating under vacuum (and this might lower the decomposition temperature). If it's a waste container, you're likely to get some carbonized gunk as well. Make sure to do this in a vessel you don't care about.



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 1-3-2016 at 18:52


This is a good question, I have collected much Pd crud over the years, and have lots of old bits of bad catalysts, I have been curious how practical it would be to combine and reuse. I have even wondered about just burning it all, then dissolving somehow and putting on carbon to reduce via hydrogenation for Pd/C catalyst. Just not sure how to do that.
View user's profile View All Posts By User
DJF90
International Hazard
*****




Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline

Mood: No Mood

[*] posted on 2-3-2016 at 16:13


Quote: Originally posted by Dr.Bob  
This is a good question, I have collected much Pd crud over the years, and have lots of old bits of bad catalysts, I have been curious how practical it would be to combine and reuse. I have even wondered about just burning it all, then dissolving somehow and putting on carbon to reduce via hydrogenation for Pd/C catalyst. Just not sure how to do that.


Please find attached some scanned pages to assist you in your endeavours. If you're aiming for Pd/C as a final product, then proceed via palladium chloride and follow existing methods for reduction on inert support material (see http://www.orgsyn.org/demo.aspx?prep=CV3P0685).

Attachment: Palladium recovery 03-Mar-2016 00-04-31.pdf (1MB)
This file has been downloaded 289 times

[Edited on 3-3-2016 by DJF90]
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: No Mood

[*] posted on 4-3-2016 at 11:27


Thanks, that is a great paper, I have never seen it mentioned before. I wish I had saved all of the Pd waste from a few years back when I used a lot of it. It went to a waste company, where they may have recovered it, but not sure. Likely not worth it for small amounts.
View user's profile View All Posts By User

  Go To Top