Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Noob trying to understand a process to know WHAT I am dealing with
silverforgestudio
Harmless
*




Posts: 4
Registered: 25-3-2015
Member Is Offline

Mood: Tinkering with conventions and the rules of money

[*] posted on 23-4-2015 at 11:29
Noob trying to understand a process to know WHAT I am dealing with


I am new to the forums... yes.

Have you read BFESSERs sticky on Silver?
-Yes... in fact- I LOVE the statement "majority of questions seem to be coming from those who have little to no interest in chemistry, but who greedily seek wealth through spoon-feeding. As a result, don't expect any mercy. There are plenty of resources out there for those who care not about the science, but only wish to refine silver for profit. Seek those out, and please spare us the nuisance."

Why am I here? Well I am dealing with a product I did not create- but know the conditions it was created under- and want to understand what I am dealing with.

I have been given the contents of an etching tank from a small jewelry shop that has closed down. Fellow used this tank for etching silver (sterling only- no gold) with his variac.

Tank was filled with Ospho (75% phosphoric acid) and DH20. (Per the owner).

The Silver was "electro-etched" and the sludge is a blackish flake.

Am I dealing with a silver phosphate or is the color from the reaction of the Cu to the acid?

I am trying to understand what is IN the tank as a product of the electro chemistry before I go mucking about trying to reclaim any of it.

Hoke and Bedford have no info regarding phosphates of silver in reclaim or purification and the flakes are the wrong color to be true silver phosphate (in my experience they are yellow orange).

Any thoughts appreciated (applying to this problem) or pointers to the direction I need to head.

Thanks in advance and I hope you guys/gals and folks have a good day!

Silver
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 23-4-2015 at 13:35


A photo or two would be helpful.



View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2015 at 14:26


Quote: Originally posted by silverforgestudio  
The Silver was "electro-etched" and the sludge is a blackish flake.



Try and dissolve some of it in % 50 nitric acid. If it dissolves easily you have elemental silver.




View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 23-4-2015 at 14:36


erm, don't many thing dissolve easily in HNO3 ?



View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4334
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 23-4-2015 at 14:48


Try dissolving it in ammonia- silver salts will generally dissolve in that. If it turns blue, it's a copper salt. If it doesn't dissolve, then try the nitric acid.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Marvin
National Hazard
****




Posts: 995
Registered: 13-10-2002
Member Is Offline

Mood: No Mood

[*] posted on 24-4-2015 at 10:20


It's a good bet the sludge is a mix of silver metal, oxide and orthophosphate with other metal salts. If a solution can be made with a small amount of nitric acid to dissolve the oxide and metal (Toxic fumes!) and then aq strong ammonia, then adding formalin should reduce the silver (and potentially any other precious metals and copper). IIRC all jewellery silver contains copper, so after the ammonia is added it will probably be deep blue.

Working with these reagents if the process fails and something more complicated is going on then they can be boiled off (outside) without adding to the bulk. Some ammonium nitrate would be formed, so you would not want to heat >100C.