Loading [MathJax]/jax/output/HTML-CSS/fonts/TeX/fontdata.js
Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Fehlings and Cu2O...
kyro8008
Harmless
*




Posts: 32
Registered: 24-8-2005
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 14-1-2006 at 07:29
Fehlings and Cu2O...


I had a load of spare rochelle salt and made up a fair amount of fehlings solution in an attempt to obtain some Cu2O - (using glucose). It worked fine; I had to use about 5 layers of filter paper to get the Cu2O out though. Unfortunately the Cu2O proved hard to get form the filter paper and it was a total failure. However I made some interesting observations and just wondered if anyone knew why:

1. I did a few different runs one after the other; the precipitate in one of the experiments was much darker - brown even compared with the other runs which were orange. Is this due to Cu2O being oxidised to CuO? - (it might have been left in longer).

2. After filtering, the filtrate was a deep orange colour and red in the run with the brown precipitate. Is this due to very fine particles of Cu2O giving it that colour? It looked like a solution to me not a suspension...

Thanks in advance.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 14-1-2006 at 09:30


I would expect colloidial Cu2O to be yellow to orange, not deep orange to red, but YMMV. You might have better luck adding the reducing agent slower, so as to make larger crystals of Cu2O (it'll probably look brick red).

Let it settle, if it doesn't form a sludge on the bottom, it must be something really weird!

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 14-1-2006 at 09:30


Cu<sub>2</sub>O indeed has many colors. See woelen's post in this thread.
View user's profile View All Posts By User
kyro8008
Harmless
*




Posts: 32
Registered: 24-8-2005
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 17-1-2006 at 10:06


thanks for the information; when I get some time ill try a few more variables and see how it goes..
View user's profile View All Posts By User
akre
Harmless
*




Posts: 16
Registered: 19-1-2004
Location: Sweden
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2006 at 10:14


I was doing Cu2O but with Benedict's solution. I later discovered that I could use fructose as the complexing agent leaving out the sodium citrate.

As for the colours, I get all colors from green to dark red depending on the ratio of Cu(II) and Cu(I). Heating slightly usually brings the reaction to dark red.

[Edited on 23-1-2006 by akre]
View user's profile View All Posts By User
CherrieBaby
Hazard to Self
**




Posts: 91
Registered: 4-3-2005
Location: London
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2006 at 14:56


If one is using it on a preparative scale the dilutions used in normal Bendict's or Fehling's 'recipes' aren't needed are they? CuSO4, tartrate and NaOH are all very soluble (if not miscible) in water. Those high dilutions are used because Bendict's and Fehling's are nearly always used an analytical reagents.
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 26-8-2008 at 14:41


Recently vacationing in Montana I learned about the smelting of copper sulfides that formerly took place in Anaconda. This inspired me to make some cuprous oxide from copper sulfate using Fehling's solutions and dextrose as reductant. I know this isn't likely the most efficient way to do it but it works nicely. My yield was only 75% as I was working on a fairly small scale. Here's a picture of my 1 gram of product:

[Edited on 26-8-2008 by Magpie]

Cu2O.jpg - 72kB
View user's profile View All Posts By User
chemkid
Hazard to Others
***




Posts: 269
Registered: 5-4-2007
Location: Suburban Hell
Member Is Offline

Mood: polarized

[*] posted on 26-8-2008 at 17:34


Perhaps try centrifuging to seperate the Cu2O from the liquid. I know most don't have access to a centifuge (myself included), but a simple two cylinder one could be made with a dremel, a bolt a small piece of metal sheet, a drill and some centrifuge tubes.

Chemkid




View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 26-8-2008 at 17:55


I separated the Cu2O from the mother liquor using a Buchner funnel and filter paper, dryed this in an oven, then scraped off the powder, without any difficulties.

I titrated the hot stirred Fehling's solution with dextrose (glucose) until the blue color was gone. The liquor color was a faint green then. When I turned the stirrer off the Cu2O quickly settled to the bottom of the beaker. The amount of dextrose required was just a little more than the theoretical 0.005g/ml of Fehling's solution.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8084
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 26-8-2008 at 23:08


One way to get a more coarse precipitate is to have very slow reduction. I also made some Cu2O from glucose and Fehling's solution, but I did this in the cold, standing at a cold place overnight. The precipitate you get in that case is brick red (like Magpie's) and fairly heavy, it quickly settles. I separated the precipitate simply by repeated decanting and shaking with distilled water. After 4 rinses, it is clean and then you can let it dry on a petri dish. After drying you can scrape off the solid. It also is remarkably compact. Five grams of solid is only a very small amount in terms of volume, the powder is fluffy, but compact.

I also made bright yellow Cu2O, this can be made easily, but hardly can be separated, as the precipitate is slimy and very voluminous. It hardly settles at the bottom. Quick formation of Cu2O can be achieved with a strong reductor, like ascorbic acid. Too strong a reductor (e.g. hydrazine) does not work, then you get metallic copper.

[Edited on 27-8-08 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
daragh8008
Hazard to Self
**




Posts: 61
Registered: 15-10-2008
Location: Eire
Member Is Offline

Mood: Happy

[*] posted on 23-2-2011 at 14:48


Sorry to bring up such an old thread, but I have been trying the last few days to make a known concentration of cucl in HCl. Since I found that the cucl tended to decompose before it had even been dried (made from cu ii salt and nacl sodium metabisulfite) I though it would be easier to weigh out cu2o and dissolve up in HCl. The cu2o I made from copper nitrate and ascorbic acid in a 1:1 molar ratio. A few goes gave me a brown mud impossible to filter. When one batch did work giving a deep red, I tried dissolving about 100mg in 36% HCl. Only a tiny fraction dissolved giving a deep yellow soln, the rest refused to dissolve. I gave up after adding 30ml of HCl and boiling for 20 mins. Am I missing something here. I though cu2o was fairly soluble in HCl. Perhaps the cu2o was mostly cu? Any suggestions. I could't find any details for the reduction of copper 2 salts with ascorbic acid so I just went 1:1. Has anyone tried this.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 24-2-2011 at 12:44


kyro8008: perhaps peptisation occurred?
View user's profile View All Posts By User

  Go To Top