TeTeC
Harmless
Posts: 4
Registered: 23-9-2005
Location: Bertrix
Member Is Offline
Mood: No Mood
|
|
CuSO4 solubility request
Hello everybody...
I'm trying to grow CuSO4 crystals. For the moment it works quite well, but I'd like to have more accuracy in my experiments.
That's why I'm asking you if you know a website, or anything that could give me the solubility of CuSO4 as a function of the temperature.
I didn't find anything with the search tool.
Thanks a lot !
|
|
Polverone
Now celebrating 21 years of madness
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline
Mood: Waiting for spring
|
|
From Lange's Handbook of Chemistry:
solubility of copper sulfate pentahydrate, in grams of solute per 100 grams of water at the specified temperature in degrees Celsius:
23.1 at 0
27.5 at 10
32.0 at 20
37.8 at 30
44.6 at 40
61.8 at 60
83.8 at 80
114 at 100
PGP Key and corresponding e-mail address
|
|
TeTeC
Harmless
Posts: 4
Registered: 23-9-2005
Location: Bertrix
Member Is Offline
Mood: No Mood
|
|
That helps, that's all I needed. ;-)
Thanks again !
|
|