Recovering Ag from E-6 process
hi
I use a 3 baths color slide developer kit from Tetenal.
this include a bleach fixer in a bath mix.
how I can recover the silver from this soup of chemicals?
http://en.wikipedia.org/wiki/E-6_process
|
|
Metacelsus
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
The silver will be complexed to EDTA. If you want metallic silver, you could try electrodepositing it.
|
|