Author: Subject: Making a metal-burning battery
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 8-8-2005 at 17:35
Making a metal-burning battery


So I want ZnO for glaze/glass flux (with a tinge of Co or Mn, it makes wonderful crystalline (Zn2SiO4) patterns! :D), how to make it? And instead of wasting the potential energy there, why not burn it electrochemically and run say a chlorate cell with the energy?

Any thoughts on electrolyte, electrode geometry, expected current density etc?