Reaction of nickel/copper alloy with hydrochloric acid
Yesterday, I dropped 10 US nickels (I believe that they're 25% nickel, 75% copper) into 60mL of ~35% hydrochloric acid. I was hoping that the nickel
would be dissolved out, leaving copper gause, and a solution of nickel chloride. But that did not happen. This morning, I checked on it. The coins did
not appear to have been corroded the slightest. The solution of hydrochloric acid had turned to the familiar and distinct yellow color of elemental
chlorine. This is what I think is happening: the hydrogen from the HCl is bonding to the surface of the coin, due to nickel's affinity for hydrogen,
causing elemental chlorine to form; and the copper causes the hydrogen to be gradually released from the nickel.
Very interesting. Perhaps this could be used to prepare elemental fluorine via non-electrolytic means from anhydrous hydrogen fluoride!
I weep at the sight of flaming acetic anhydride.
|
|
Blind Angel
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 845
Registered: 24-11-2002
Location: Québec
Member Is Offline
Mood: Meh!
|
|
just to know, nickel and copper doesn't oxydize on coins?
/}/_//|//) /-\\/|//¬/=/_
My PGP Key Fingerprint: D4EA A609 55E4 7ADD 8529 359D D6E2 33F6 4C76 78ED
|
|
Polverone
Now celebrating 21 years of madness
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline
Mood: Waiting for spring
|
|
I think your imagination is running ahead of your experiments again :-) First of all, nickel is more active than copper, so it is the nickel that
would be dissolved, leaving copper behind, if this reaction had worked how you had hoped.
I've tried dissolving nickels in HCl myself. The surface quickly acquired a sort of dull matte color - presumably from dissolution of the nickel - and
then didn't do much for a long time, since copper doesn't dissolve in pure HCl very well at all. You can speed up the reaction (as I'm sure you know)
with the addition of H2O2.
I think you are jumping to conclusions about the source of yellow in your HCl, as well. Technical grade acid contains considerable impurities. I have
often seen it turn yellow in various reactions, whether or not chlorine is being generated. Nickel is higher in the electromotive series than
hydrogen, so I'm sure it would react with HF to form nickel fluoride and hydrogen gas, assuming the surface did not become passivated.
[Edited on 6-30-2014 by Polverone]