Hi, i need copper in dust and i think that 2HCl + Cu -----> CuCl2 + H2 and then CuCl2 + Al ------> Cu + AlCl2 and then remove the AlCl2... is
it possible???
thanks
Sorry by the new topic but i havenĀ“t found anything...
[Edited on 16-1-2005 by sathor]
|
|
neutrino
International Hazard
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
It would be AlCl<sub>3</sub>, not AlCl<sub>2</sub>. This could work, as aluminum chloride is soluble. There is another thread on this where CuSO<sub>4</sub> and Vitamin C is used.
|
|
cyclonite4
Hazard to Others
Posts: 480
Registered: 16-11-2004
Location: is unknown
Member Is Offline
Mood: Amphoteric
|
|
HCl doesnt react directly with Copper, the Cu has to be oxidised first, so you could react the oxide with acid, add an oxidising agent, or bubble air
through the acid to aid dissolving the Copper.
\"It is dangerous to be right, when your government is wrong.\" - Voltaire
|
|
chemoleo
Biochemicus Energeticus
Posts: 3005
Registered: 23-7-2003
Location: England Germany
Member Is Offline
Mood: crystalline
|
|
THere's a multitude of threads on copper dissolution and so on. If'd like to discuss this please do so in the proper threads. Same goes for
the copper powder - just follow neutrino's link.
Btw - Zn, and Fe powder was mentioned for the production of Cu powder. Al presumably should work too.