Help improving the process
Hello,
Please forgive this double posting. I can't figure out any
other way to get my request for possible suggestions
or help up on top so people can see it.
This is in reference to my other topic about
"Making Edison Cylinder Records".
In short, it involves saponifying stearic acid with NaOH.
I am looking for ways to make a condensor/separator
to recover the stearic which normally boils away.
Please see my other post, scroll to the bottom.
I have a link to a video that shows how I'm doing it
now.
Thanks!!
"Opportunity is missed by most people
because it is dressed in overalls and it
looks like work" T.A. Edison
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Feed it through a tube into a flask in a cold or ice water bath.
|
|
HgDinis25
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 439
Registered: 14-3-2014
Location: Portugal
Member Is Offline
Mood: Who drank my mercury?
|
|
You coud lead it through a tube directly into could water. Stearic Acid has a very low solubility in water (3 mg/L (20 °C)).
And where's your other post? There's no link...
|
|
sodium_stearate
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 22-4-2011
Location: guard duty at the checkpoint
Member Is Offline
Mood: No mask.
|
|
Thanks for that suggestion. One consideration there would
be to manage the temperature in the tube somehow
so that the stearic would stay liquid, thus somehow then
being returned to the main vessel, maybe dripping back
down in there.
Meanwhile the water vapor condenses and drains away.
I've given this considerable thought, and it's not a real
simple thing.
Ideally, the entire process could be sealed. But then it
starts getting complicated because it needs to be looked
at, stirred, and caustic solution added slowly, portionwise.
"Opportunity is missed by most people
because it is dressed in overalls and it
looks like work" T.A. Edison
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
You've just described a reflux! Search "Reflux" on Wikipedia for more help! It also cannot be sealed, the pressure will make it explode.
|
|
sodium_stearate
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 255
Registered: 22-4-2011
Location: guard duty at the checkpoint
Member Is Offline
Mood: No mask.
|
|
Here's the link:
http://youtu.be/LrR9h9fu324
and thanks again smug!![:cool:](./images/smilies/cool.gif)
Yes, I know the steam pressure would build up if
it were sealed, and that's been a part of my thinking about this
for a long while now. Some pressure would probably
benefit the process, but it would need to be controlled
to a set pressure by some sort of a relief or safety valve.
"Opportunity is missed by most people
because it is dressed in overalls and it
looks like work" T.A. Edison
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
You're welcome!
|
|