Torch for melting and heating glass
Earlier today I was melting down some bismuth (very fun), but the plastic on my butane burner cracked from its own heat which in turn broke the gas
valve. I was going to make some Hexaaminenickel(ii) chloride and store it in an ampule, but now I have no way of sealing said ampule. I have
seen videos of people melting and heating glass with handheld burners (not like blow torches, more like lighters) and was wondering what type of
burner/torch would provide adequate heat to melt glass (or at least soften it a reasonable amount).
[edit] I don't mean to make a spoonfeeding request, so if this is too spoonfeed-y just tell me.
[Edited on 2/18/14 by thesmug]
|
|
froot
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 347
Registered: 23-10-2003
Location: South Africa
Member Is Offline
Mood: refluxed
|
|
Something like this:
![](http://www.gasproducts.co.uk/acatalog/B110P.jpg)
http://www.gasproducts.co.uk/acatalog/Bullfinch_Torch_Kits.h...
We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Do you know of anything thats like that but a bit more portable?
|
|
hyfalcon
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Try one of these. You can use propane or mapp gas cylinders.
http://www.bernzomatic.com/item.html?id=15
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Of the two fuel types which would be better?
Would one of these work?
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
MAPP gets to a much higher flame temperature, propane is cheaper, depends on your situation.
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Well cheaper is always better. What about those Butane torches?
|
|
hyfalcon
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
Not enough heat if you want to melt glass together.
|
|
thesmug
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Ok, thanks. I just remembered that I have a torch laying around I just don't have any fuel canisters.
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
I think butane could melt glass, it would take longer and more fuel though. Also isn't propane cheaper?
|
|
Electra
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 179
Registered: 11-12-2013
Member Is Offline
Mood: No Mood
|
|
You can get propane, butane, and acetylene/oxygen torches all at home depot. All should be able to melt glass. To my knowledge propane only burns 20
degrees hotter than butane so a small butane torch might suit your purposes perfectly. Home depot and other hardware stores should carry them in all
sorts of sizes
|
|