PETN mixed with Sylguard 182 in a 4 to 1 ratio of nitrate to polymer produces a material that can be extruded out of a caulking gun and set via heat.
I would like to know more about these use forms. I'm considering a mix using 85% nitromannitol and 15% Sylguard 184 (the 182 seems to be mil spec and
unavailable to the general public at reasonable prices).
What kind of force would be necessary to initiate such a mixture?
[Edited on 26-9-2013 by killswitch]
|
|
|
malford
Hazard to Others
 
Posts: 116
Registered: 17-6-2013
Member Is Offline
Mood: No Mood
|
|
Please explain the purpose of diphenylamine.
|
|
|
killswitch
Hazard to Others
 
Posts: 209
Registered: 8-7-2011
Location: is a relative concept
Member Is Offline
Mood: No Mood
|
|
Stabilizer. It absorbs evolved NO2.
Though I'm unsure if it's necessary in this case.
|
|
|
Rosco Bodine
Banned
Posts: 6370
Registered: 29-9-2004
Member Is Offline
Mood: analytical
|
|
cyanoguanidine is a better stabilizer for nitromannite
|
|
|
Ral123
National Hazard
  
Posts: 735
Registered: 31-12-2011
Member Is Offline
Mood: No Mood
|
|
Isn't urea and carbonates also good? Some knows the storage stability of MHN?
|
|
|
Dany
Hazard to Others
 
Posts: 482
Registered: 3-8-2013
Member Is Offline
Mood: No Mood
|
|
The answer on this problem is impossible in your situation. Nothing is known about the physical properties of your material. Even if all physical
parameters are known, the sensitivity of the material will change from test to another and may not be reproducible even in the same test. the reason
for this is that sensitivity is a complexe feature of an HEDM (see B. Dobratz, PROPERTIES OF CHEMICAL EXPLOSIVES AND EXPLOSIVE SIMULANTS, 1972)
You may want to make some test on your new explosive to deduce the ''force'' needed for initiation. for example, you can make many blasting cap
containing different amount of initiating explosive. by detonating several charge with these initiators (the charge are put on a witness plate for
detonation confirmation) you can deduce some information on the force needed for initiation. You can compare the result to another reference explosive
that you have tested with the same blasting cap. but you should keep in mind that the charges need to be carefully made, this mean all charges should
be the same (same loading density, confinement, granulometrie...) or your result will suffer from large errors leading to erroneous conclusion.
Dany.
|
|
|
golfpro
Banned
Posts: 179
Registered: 18-5-2013
Member Is Offline
Mood: Cap Sensitive
|
|
plasticized ETN with enough plasticizer to hold it together, (90% and 10%) but still no different texture or feel than gum already been chewed is
water proof and sensitive to a hammer strike.
|
|
|