Interesting...I just read of some research, where scientists have prepared ultra thin nanowires of 10-20 nm wide composed of silicon with a sillicon
oxide coating.
These wires are stable in air for a long time, nonflammable, and yet, when hit with a reasonably intense flash from a camera they ignite with a loud
crack.
they were made by sealing sillicon monoxide or a one to one mixture of silicon and sillica inside of an air free quartz tube, of which one end was
heated in a furnace for 30 minutes at 1200-1300 C, and these Si nanowires form on the part of the tube outside of the furnace at temperatures of from
800 to 1000 C.
Sounds like this might be a project for axehandle with his metal melting furnace
The sun is shining on a brand new day
Blackened corpses burn where they were slain
Self-flagellation prompts him to confess, Bless me father, for I made this mess.
|
|
Esplosivo
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 491
Registered: 7-2-2004
Location: Mediterranean
Member Is Offline
Mood: Quantized
|
|
If he manages to draw out a silicon wire with such a thickness he will personally become my idol. I think 20nm is a little too thin
to do it home-made right? ![:P](./images/smilies/tongue.gif)
Anyway the fact is that what occurs is really interesting, though I haven't fully understood how it works. If the Si wire is coated by an inert
layer of SiO2 how does the internal layer of Si ignite?
And btw, you mentioned SiO. Well using SiO2 (quartz) I would have imagined that the latter can be used for oxidising the Si forming SiO. But in the
case of SiO, it cannot give up the O to an Si atome right? If I remeber correctly SiO is very unstable?
[Edited on 7-8-2004 by Esplosivo]
Theory guides, experiment decides.
|
|
IvX
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 112
Registered: 14-4-2004
Member Is Offline
Mood: No Mood
|
|
Quote: | Originally posted by Esplosivo
Anyway the fact is that what occurs is really interesting, though I haven't fully understood how it works. If the Si wire is coated by an inert
layer of SiO2 how does the internal layer of Si ignite?
[Edited on 7-8-2004 by Esplosivo] |
Electroplosion probably.Google will give you a lot of results but basically it's when electrons(I think) "flood"the material so it
litrelly blows up like an overfilled ballon.
With normal wires you need a LOT of juice dumped in a VERY short time but considering the tiny size and that things do behave diferently at that size
it's almost certain that thats what hapening.
|
|
vulture
Forum Gatekeeper
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
Pure silicium oxide does not stop the high energy UV rays of a flash.
As Si is a semiconductor this foton bombardment will knock quite a few electrons into an excited state, IMHO.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Reduction of SiCl4 in a hydrogen atmosphere with a hot tungsten filiment? That is the usual procedure for making boron fabrics and such, although I
doubt you are going to find a tungsten filiment as fine as you would need to deposit a layre of silicon and still be so incredibly small.
|
|
Nick F
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 439
Registered: 7-9-2002
Member Is Offline
Mood: No Mood
|
|
"they were made by sealing sillicon monoxide or a one to one mixture of silicon and sillica inside of an air free quartz tube, of which one end
was heated in a furnace for 30 minutes at 1200-1300 C, and these Si nanowires form on the part of the tube outside of the furnace at temperatures of
from 800 to 1000 C."
Sounds like they form themselves.
|
|
Reverend Necroticus Rex
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 196
Registered: 15-6-2004
Location: Right behind you.......
Member Is Offline
Mood: Poisonous
|
|
Apparrently, there is also a form of nano-carbon that behaves the same way.
An interesting point about these nanowires is that they don't flash and burn in argon/inert of your choice, but the Si core is still vaporised
out, leaving tiny nanotubes of the casing.
And Nick F is right, AFAIK the wires sublime onto the cooler part of the tube that is outside of the furnace.