[*] posted on 2-4-2013 at 02:19
Basifying Agents


Hi,

I am wondering about choice of basifying agents / solutions.
I have seen sodium hydroxide and ammonium hydroxide used for basifying in liquid-liquid extractions.

I was just wondering when is best to use each of them.
To me it seems like an arguement of weak vs strong bases but is there anything else to the story?

Cheers, Houngan




The spice must flow.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8149
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 2-4-2013 at 02:33


NaOH only adds base and Na(+) ions to your solution, ammonia also adds NH3. The latter can react with many compounds, can dissolve in other solvents than water (e.g. when extracting things) and it can form coordination complexes with many metals. So, yes, there is more to it than just the strength of the base. Other suitable weak bases may be sodium acetate, sodium carbonate. It just depends on what you really want.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Houngan
Harmless
*




Posts: 16
Registered: 19-1-2012
Location: Space
Member Is Offline

Mood: Regioregular

[*] posted on 2-4-2013 at 15:33


Thanks woelen!

So is the NH3 required for extraction of alkaloids?

Cheers, Houngan




The spice must flow.
View user's profile View All Posts By User
Houngan
Harmless
*




Posts: 16
Registered: 19-1-2012
Location: Space
Member Is Offline

Mood: Regioregular

[*] posted on 7-4-2013 at 00:55


What would be a good system to practice one?

Cheers, Houngan




The spice must flow.
View user's profile View All Posts By User
DJF90
International Hazard
*****




Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2013 at 01:42


There are a whole variety of solutions available for work up. Generally theres strong/weak acid/base solutions, and some other more specialist solutions.

Saturated sodium bicarbonate has a pH of 8 and will wash acidic compounds into the aqueous layer. It provides a means to remove unreacted acid from an esterification reaction (for example) facilitating isolation of relatively pure material. It is also used for neutralizing an acidic solution, as the pH will only ever rise to pH 8.

Sodium hydroxide (various concentrations) is used to basify in liquid-liquid extraction. It will bring the pH to 12-14 quite readily, allowing the extraction of free amines from the aqueous phase. It is often used occasionally for working up zinc-based reductions, as the soluble zinc (II) first precipitates (do it before transfer to the sep funnel!) and then dissolves as an excess of NaOH is added (as sodium zincate). Its also used in the famous Feiser workup for LAH reductions.

Aqueous ammonia is often used as a 5 or 10%w/w solution. It has use for washing organic extracts from reactions utilising copper salts, amongst other metals. The aqueous layer turns blue (in the case of copper) and when subsequent washes remain colourless you can be fairly confident theres no copper left. I used this a load when I was doing Stille couplings with CuI as a co-catalyst.

I could elaborate on other solutions but it depends if theres a demand for such info. Much can be gleaned from the not-voodoo site (uni rochester).