Hello, I am looking to make some Potassium Chlorate using electrolysis and I am unable to find any salt that is completely free of Sodium Chloride.
I'm thinking that I could seperate them with different solubilities but then I'd lose alot of it.
Or... I could just make a solution of it without seperating.
Now, I'm thinking that would just make Potassium Chlorate and the sodium chloride would just make chlorine and hydrogen.
Am I wrong? Will the sodium chloride interfere with the electrolysis?
|
|
plante1999
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
This is the wrong section, I have seen people using 55% KCl 45% NaCl without problems. I would be more preoccupied by your anode and cathode tough...
I never asked for this.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
The potassium chlorate does precipitate out, correct? If that's the case, you shouldn't have much of a problem (the sodium chlorate will just stay in
solution).
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Manifest
Script Kiddie Asshole
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 7-12-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by plante1999 ![](images/xpblue/lastpost.gif) | This is the wrong section, I have seen people using 55% KCl 45% NaCl without problems. I would be more preoccupied by your anode and cathode tough...
|
What section do you suggest it should be in then?
Maybe 2 Carbon electrodes.
Or copper.
|
|
m1tanker78
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 685
Registered: 5-1-2011
Member Is Offline
Mood: No Mood
|
|
Graphite/carbon has worked well for me. The anode shreds quite a bit but is easily filtered through clean sand or vac filtered if available.
You're across the pond but around here, I can buy 50 pound bags of pure KCl at a supermarket (intended for water softener). Been a while but don't you
need to start with NaCl unless you're using platinum or lead dioxide?? I might be confusing perchlorate but am too lazy to check. Bah!
Tank
Chemical CURIOSITY KILLED THE CATalyst.
|
|
Manifest
Script Kiddie Asshole
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 7-12-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by m1tanker78 ![](images/xpblue/lastpost.gif) | Graphite/carbon has worked well for me. The anode shreds quite a bit but is easily filtered through clean sand or vac filtered if available.
You're across the pond but around here, I can buy 50 pound bags of pure KCl at a supermarket (intended for water softener). Been a while but don't you
need to start with NaCl unless you're using platinum or lead dioxide?? I might be confusing perchlorate but am too lazy to check. Bah!
Tank |
:? Why not filter paper?
I don't think so. Don't really understand what you mean.
I wonder would Potassium Chlorate and Sugar rockets work as well as the potassium nitrate and sugar ones do.
|
|
m1tanker78
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 685
Registered: 5-1-2011
Member Is Offline
Mood: No Mood
|
|
Coffee filters will pass some carbon sludge and become clogged. I suppose you can use a commercial buchner funnel paper but if you don't have a vac,
be prepared to wait for a long time. Clean sand or quartz or 'silica' can be packed on top of your coffee filters to greatly speed up gravity
filtration and prevent the filters from becoming clogged. Doing so yields a perfectly clear filtrate.
UTFSE and read the dozens of picture tutorials out there.
Tank