Question regarding a thermite
been looking around. Any termite which is self igniting (maybe through an initial slow reaction or drying). Thanks.
|
|
Oscilllator
National Hazard
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
thermites are usually pretty hard to set off, although a sparkler almost always does the job.
Also, since when did you dry out thermites? If your using aluminium powder as a fuel, the water may well create an oxidised layer on the aluminium
powder which will make the thermite harder, not easier, to detonate.