Metal melting points


What are the melting points of tungsten and molybdenum? I keep getting conflicting information on the net,
I have heard both 1650 C and 3370 and 3410 C for tungsten, and 2623 C for molybdenum, which of these is correct, or are there any metals/alloys with even higher Mp ?




Sweet dreams are made of her
slit my wrists and dissappear
I am no-one any more
I wear my crown of thorns in view of all
View user's profile View All Posts By User This user has MSN Messenger
axehandle
Free Radical
*****




Posts: 1065
Registered: 30-12-2003
Location: Sweden
Member Is Offline

Mood: horny

[*] posted on 12-6-2004 at 07:31


3410C for W.
2623C for Mo.

3652C is the sublimation point of C.




My PGP key, Fingerprint 5D96 E09E 365D 1867 2DF5 C2FE 4269 9C19 E079 CD35

\"Verbing nouns weirds the language!\"
View user's profile View All Posts By User

  Go To Top