I notice that silver electrodes eventually turn black. The black stuff must be silver oxide (AgO2). Silver oxide is a mild oxidising agent
so I tried soaking the electrodes in a solution of sodium metabisulfite (a reducing agent) but no reaction occurs. Would I have better luck by soaking
them in an acid?
|
|
hissingnoise
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3940
Registered: 26-12-2002
Member Is Offline
Mood: Pulverulescent!
|
|
Most probably! Dilute HNO<sub>3</sub>, most likely . . .
|
|
barley81
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 481
Registered: 9-5-2011
Member Is Offline
Mood: No Mood
|
|
Clean them like you clean tarnished silver in the kitchen: dissolve some baking soda in water, put an aluminum foil sheet in the solution, and then
drop in the silver. The aluminum reduces the silver compounds that are adhering to the silver.
@hissingnoise when did you stop being Pulverulescent?
[Edited on 6-5-2012 by barley81]
|
|
phlogiston
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
The black layer is usually silver sulfide actually. Silver does not tarnish in oxygen.
-----