GreenD
National Hazard
  
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
ZnCl2 from ZnO?
Hello!
It would seem that ZnCl could be made from ZnO and HCl. The other product being water.
Has anyone carried this out? How concentrated does the HCl have to be? I have 1N (damn bio people!) HCl with some ZnO. I have read that heat isn't
necessary as the ZnCl will spontaneously form - but removal of water should help.
Any tips on this simple reaction?
ʃ Ψ*Ψ
Keepin' it real.
Check out my new collaborated site: MNMLimpact.com
|
|
|
Adas
National Hazard
  
Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline
Mood: Sensitive to shock and friction
|
|
You can use any concentration. Be sure to react all ZnO and then evaporate water. How simple.
Rest In Pieces!
|
|
|
GreenD
National Hazard
  
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
Yay! This is my first chemical reaction. How neat 
And - it should be easy to gauge. ZnCl2 is soluble in water, while ZnO is not. Oh what a wonderful reaction.
ʃ Ψ*Ψ
Keepin' it real.
Check out my new collaborated site: MNMLimpact.com
|
|
|
Nicodem
Super Moderator
     
Posts: 4230
Registered: 28-12-2004
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Adas  | | You can use any concentration. Be sure to react all ZnO and then evaporate water. How simple. |
Please, provide the reference. If it would be so simple to prepare zinc chloride, I don't see why researchers developed so many much more complicated
methods to prepare it.
Not only it dissolves in water, it also decomposes. It is not trivial to regenerate pure enough ZnCl2 from its aqueous solution.
…there is a human touch of the cultist “believer” in every theorist that he must struggle against as being
unworthy of the scientist. Some of the greatest men of science have publicly repudiated a theory which earlier they hotly defended. In this lies their
scientific temper, not in the scientific defense of the theory. - Weston La Barre (Ghost Dance, 1972)
Read the The ScienceMadness Guidelines!
|
|
|
simba
Hazard to Others
 
Posts: 175
Registered: 20-5-2011
Member Is Offline
Mood: No Mood
|
|
You can always buy muriatic acid (over 30% HCl) at the hardware store.
|
|
|
Endimion17
International Hazard
   
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
You'll end up with zinc oxychloride. If you want zinc chloride, be prepared for messing with chlorine, unless you can buy the salt.
|
|
|
GreenD
National Hazard
  
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
So... I'm not going to get ZnCl2 from ZnO and HCl?
Can anyone link me to a ZnCl2 prep? I'm not very good at finding basic info- I always end up with the 2010 or 2009 papers.
Looks like (thanks AJKOER) adding KCl to the aqueous solution will cause the Zn-hypochlorite to give ZnCl and KClO3
[Edited on 6-3-2012 by GreenD]
ʃ Ψ*Ψ
Keepin' it real.
Check out my new collaborated site: MNMLimpact.com
|
|
|
LanthanumK
Hazard to Others
 
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
Zinc chloride is deliquescent. Prevention of decomposition when heated could be done by evaporating it from an HCl solution. Zinc sulfate is better
for use as a primary zinc salt.
hibernating...
|
|
|
Endimion17
International Hazard
   
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
Quote: Originally posted by GreenD  | So... I'm not going to get ZnCl2 from ZnO and HCl?
Can anyone link me to a ZnCl2 prep? I'm not very good at finding basic info- I always end up with the 2010 or 2009 papers.
Looks like (thanks AJKOER) adding KCl to the aqueous solution will cause the Zn-hypochlorite to give ZnCl and KClO3
[Edited on 6-3-2012 by GreenD] |
At best you can get a deliquescent slush of hydrated salt, which is not actual zinc chloride.
Anhydrous zinc chloride is prepared by synthesizing it from the elements, which, in homemade conditions, usually ends up with slight chlorine
poisoning.
|
|
|
GreenD
National Hazard
  
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
Damnit. ok. Internet shopping here i come.
ʃ Ψ*Ψ
Keepin' it real.
Check out my new collaborated site: MNMLimpact.com
|
|
|
Vikascoder
Hazard to Others
 
Posts: 309
Registered: 28-1-2012
Member Is Offline
Mood: No Mood
|
|
Zinc oxide is amphoteric so it will make zinc chloride with hydrochloric acid.
|
|
|
Nicodem
Super Moderator
     
Posts: 4230
Registered: 28-12-2004
Member Is Offline
Mood: No Mood
|
|
Vikascoder, please do not double-post replies. I have better things to do than the cleaning job. If you double-post by mistake make sure you delete
the repeated post by using the "Edit | Delete this post" function. Make sure you read the forum's posting guidelines.
It is highly advised to read the entire thread before posting a reply (especially if it is as short as this one!). Also in general, it would help you
immensely if you would do any reading at all.
It was already explained that dissolving zinc oxide (or zinc) in hydrochloric acid does not give zinc chloride. The only thing you get is an aqueous
solution of hydrated (decomposed) zinc chloride. Zinc chloride hydrolyzes immediately in contact with water, hence it can not be easily regenerated
from aqueous solutions (there are ways to do this, but nothing trivial: UTFSE for more info).
|
|
|
GreenD
National Hazard
  
Posts: 623
Registered: 30-3-2011
Member Is Offline
Mood: Not really high anymore
|
|
For the record I put ZnO in 1N HCl (excess). Let stir for one hour - no noticeable difference.
Heated and stirred for 3 hours - no noticeable difference.
ʃ Ψ*Ψ
Keepin' it real.
Check out my new collaborated site: MNMLimpact.com
|
|
|
LanthanumK
Hazard to Others
 
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
The oxide could be calcined and therefore resistant to acid attack.
hibernating...
|
|
|
AirCowPeaCock
Hazard to Others
 
Posts: 311
Registered: 9-1-2012
Location: In your nation!
Member Is Offline
Mood: Hazardous
|
|
GreenD did the zinc oxide "dissolve"?
BOLD
|
|
|