Author: Subject: Mg powder + Li2CO3 => ?? (I tried it)
metalresearcher
National Hazard
****




Posts: 737
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 13-11-2011 at 09:14
Mg powder + Li2CO3 => ?? (I tried it)


Mixing 0.5g Mg powder + 1g Li2CO3 and putting it in a steel retort which I heated to red hot resulted in a red flare as a result of a vigorous reaction. After allowing the retort to cool and opening it, a black powder was tht result. It did not react with water nor did it dissolve.
I hoped to get some Li metal but no avail.

What happened ?
View user's profile View All Posts By User
Adas
National Hazard
****




Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline

Mood: Sensitive to shock and friction

[*] posted on 13-11-2011 at 09:44


2 Mg + Li2CO3 ----> Li2O + 2 MgO + C
View user's profile Visit user's homepage View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 13-11-2011 at 11:31


The only real way to make lithium metal is by electrolysis. All other methods will either yield no metal or poor quality crap, embedded in slag from which it cannot be separated adequately.