Turning Li metal blocks into powder
Hello folks,
How would you turn lithium chips or ingots into a powder on a DIY scale/budget?
I am thinking that as the MP of Li is conveniently low (181C), one can melt it in a stainless steel vessel containing an inert atmosphere (e.g. He)
and pressure inject it through an atomiser into a chamber also in an inert atmosphere. Desired particle size is anything under 100 microns.
To remove the Li powder you flush the chamber with paraffin oil and get a powder metal + oil slurry.
Does anyone know if this approach will work and if it does, how I come to suitable dimensions for the nozzle given molten Li's characteristics
(viscosity, surface tension, desired particle size, etc.)
Thanks.
|
|
bbartlog
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1139
Registered: 27-8-2009
Location: Unmoored in time
Member Is Offline
Mood: No Mood
|
|
I'm not an expert on the techonology, but atomization of molten metal will probably require either pressurized gas (a stream of gas to break the
liquid into tiny droplets) or else a rapidly spinning disk on to which the molten metal is dropped (tears the drops apart using centrifugal force).
I'm not sure you can achieve the particle size you want just by pushing the molten metal through a nozzle.
However, given the low melting point of Li, I would think that if you have a solvent that it won't react with, you should be able to melt it with the
solvent and then just atomize it by blending. Paraffin oil with bp around 200C?
|
|
Fusionfire
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 219
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
Thanks. I'm not an expert on the technology as well, but we all start from the beginning ![:)](./images/smilies/smile.gif)
BTW, I picked a stainless steel reaction vessel because Fe/C/Cr/V doesn't have any intermetallic reactions with Li AFAIK.
Fischer, S. H. and M. C. Grubelich (1996). A Survey of Combustible Metals, Thermites and Intermetallics for Pyrotechnic Applications. 32nd
AIAA/ASME/SAE/ASEE Joint Propulsion Conference, Lake Buena Vista, FL.
http://www.osti.gov/bridge/servlets/purl/372665-kjTA0r/webvi...
I can build two very fine nozzles (say bore diameter 80 ga or 0.343mm). One extrudes the liquid Li injected through it, and another arranged
perpendicular to it blasts the molten Li stream with He or paraffin oil.
|
|
bahamuth
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline
Mood: Under stimulated
|
|
A Morton flask is used to create tiny beads of alkaline metal in a high bp solvent. Overhead stirrer is a must as I do nont think any magnetic
strirrer will do..
Do not know if it will create particles as small as 100 µm though.
Any sufficiently advanced technology is indistinguishable from magic.
|
|
UnclearReactor
Harmless
Posts: 9
Registered: 11-1-2008
Location: Eastern US
Member Is Offline
Mood: No Mood
|
|
Spray nozzles have a unique geometry suited to the working fluid (viscosity, density, etc). For instance, the stream impinges on a something or is
shaped like a pressure washer's or an airless paint sprayer's with a v-groove cut in it. Determining the geometry (which will change with the
pressure) may be a daunting task. Or you might get lucky. The biggest hurdle is that you will have to ensure that the droplets don't coalesce before
they freeze. Thermal stratification of the host fluid might work, but you will need a fluid lighter than lithum. Propane under pressure, maybe?
|
|
symboom
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline
Mood: Doing science while it is still legal since 2010
|
|
Vaporizing the metal is one way its up there in temperature wise is you have an oxy-fuel welder its no problem as temp reaches 6000F to heat the
bottom of an inverted u shaped tube.
barium metal is produced by barium oxide and aluminum. barium vapor is condensed into a cooling chamber water jacket if you use dry ice in acetone or
denatured alcohol as a cooling jacket it might be possable to flash solidify the lithium as a powder of course all done in a atmosphere of argon being
the cheapest. as it is pyrophoric which makes this very dangerous in vaporized state 2448 °F is lithiums boiling point condensing it into kerosene or
mineral oil sorrounded by dry ice cooling jacket
|
|
Sedit
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1939
Registered: 23-11-2008
Member Is Offline
Mood: Manic Expressive
|
|
Lithium nitride synthesis - US2910347
I can't remember the partical size it generated but it was fine enough so that Lithium and N2 reacted in good yields, the speed of stirring must be
very high however. Replace N2 with argon in this case.
[edit]
Its stated the average particle size was slightly under 100microns.
[Edited on 6-11-2011 by Sedit]
Knowledge is useless to useless people...
"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the
fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story
before."~Maynard James Keenan
|
|
Yamato71
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 68
Registered: 8-2-2012
Member Is Offline
Mood: Resigned
|
|
You might try grinding a mixture of dry ice and lithium metal in a coffee grinder until the metal is of the desired particle size. At the temperature
of dry ice, the normally soft waxy metal becomes brittle and shatters like glass. Under a microscope, these fragments will be bright, jagged and
crystalline, with a greatly increased surface area. Consequently, it will be more reactive, so you might want to add a bit of mineral oil or a spritz
of WD-40 to the mix before grinding. You must then allow the dry ice to sublime by wrapping the coffee grinder in a towel and placing it in a freezer
with the lid loosely in place. If you try to sublime the dry ice outside of a freezer, frost will form on the inside of the grinder and react with
the lithium when it melts, possibly starting a fire. Let us know if this works.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Quote: Originally posted by Yamato71 ![](images/xpblue/lastpost.gif) | You might try grinding a mixture of dry ice and lithium metal in a coffee grinder until the metal is of the desired particle size. At the temperature
of dry ice, the normally soft waxy metal becomes brittle and shatters like glass. Under a microscope, these fragments will be bright, jagged and
crystalline, with a greatly increased surface area. Consequently, it will be more reactive, so you might want to add a bit of mineral oil or a spritz
of WD-40 to the mix before grinding. You must then allow the dry ice to sublime by wrapping the coffee grinder in a towel and placing it in a freezer
with the lid loosely in place. If you try to sublime the dry ice outside of a freezer, frost will form on the inside of the grinder and react with
the lithium when it melts, possibly starting a fire. Let us know if this works. |
Lithium is reactive with carbon dioxide....
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Yamato71
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 68
Registered: 8-2-2012
Member Is Offline
Mood: Resigned
|
|
Not at -78c
|
|
Texium
|
Thread Moved 20-11-2023 at 12:43 |