We all know what hapens when you mix borax with glue, and get a slimey polymer... but a while back I was doing experiments- and I know aluminum is related to boron... Finially, I found the formulation.

Make a saturated solution of aluminum potassium sulphate.
Now, squeeze in PVA glue.
You now have a weird, stringy polymer.

Can anyone help identify this?




hey, if you are reading this, I can't U2U, but you are always welcome to send me an email!


View user's profile Visit user's homepage View All Posts By User
fledarmus
Hazard to Others
***




Posts: 187
Registered: 23-6-2011
Member Is Offline

Mood: No Mood

[*] posted on 13-10-2011 at 04:16


PVA is a polymer! Are you sure you don't just have glue with a lot of aluminum salts dissolved in it?
View user's profile View All Posts By User
barley81
Hazard to Others
***




Posts: 481
Registered: 9-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 13-10-2011 at 07:56


It's possible that the water was 'sucked' from the glue via osmosis, which congealed it.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 13-10-2011 at 16:29


Quote: Originally posted by ScienceHideout  
Make a saturated solution of aluminum potassium sulphate.
Now, squeeze in PVA glue.
You now have a weird, stringy polymer.

Can anyone help identify this?
You have cross-linked PVA. Google "PVA slime".