Cadmium nitrate purification...


I have some cadmium nitrate which is slightly contaminated with nickle nitrate what would be the easiest way to seperate those two.
i want better purity of cadmium nitrate...




View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 3-7-2011 at 07:43


According to my qualitative analysis scheme Cd++ will be taken down (precipitated) by bubbling in H2S in 0.3M HCl. The ppt will be CdS. Ni++ will not come down.

Separate the washed CdS and dissolve it in 6M HNO3. This should release the sulfide as H2S leaving you with very pure Cd(NO3)2.

CAUTION: This must all be done outside or in a good fume hood to avoid being fatally poisoned by H2S fumes.
---------------
Also see: http://www.sciencemadness.org/talk/viewthread.php?tid=4676#p...

[Edited on 3-7-2011 by Magpie]




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User

  Go To Top