Electrodes
Where do you guys get your electrodes from, i am looking for Ti-MMO/DSA or Platinised-Ti electrodes i tried searching ebay i cant find nothing, maybe
im not using the right keywords. Also is there a way to make platinise a ti electrode i remember seeing nurd rage make magnanese dioxide coated
electrode im wondering if there is a similar process?
|
|
sternman318
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 21-4-2011
Member Is Offline
Mood: No Mood
|
|
http://www.esslinger.com/platinizedtitaniumanode1x4mesh.aspx
http://sra-solder.com/product.php/6497/87
|
|
#maverick#
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 209
Registered: 7-4-2011
Member Is Offline
Mood: hybridised
|
|
Thank you very much
|
|