Why do explosive jelly degrade?


It jelly-like explosives made of nitroesters (NG, EGDN, DEGDN) and 7-10% coloxylin.

In many books (especially in 1930s) it is stated that freshly prepared explosive jelly yields about 7800 m/sec

But after a few days the explosive jelly produces only 2-3 km/s, and after a few years it does not initiate at all.

And then I realized that I do not know the reasons for this, in the books where this phenomenon is described there is no explanation, and more modern studies I have not found, because the explosive jelly became not interesting to society seems to be before the Second World War

[Edited on 25-7-2024 by DennyDevHE77]
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1749
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 25-7-2024 at 00:53


I assume coloxylin is cellulose nitrate?

My first guess would be the presence of bubbles/voids, these can have a significant effect on explosive performance.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
DennyDevHE77
Hazard to Others
***




Posts: 168
Registered: 15-9-2014
Member Is Offline

Mood: No Mood

[*] posted on 25-7-2024 at 01:15


Yeah. Colloxylin is cellulose dinitrate. Trinitrate is almost never gelatinized.
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1447
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 25-7-2024 at 03:07


.......DennyDevHE77........information in books are nonsenses. Quality stabilzed ( neutralized) nitroesters (and his mixtures) and nitrocompounds are stabille in order 20 years.
Similarly as is stabille nitrocellulose / nitroglycerine shotgun powder with content stabilizator centralite or nexts stabilzitators. If is mixture stabile, is not reason for decrease VoD. Yes, weak no quality detonator can cause low VoD.




Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 920
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 25-7-2024 at 09:15


I agree with all of the above. As the jelly slowly sets and becomes more homogenous, it probably becomes more prone to incomplete initiation and low order detonation if the detonator is not powerful enough. This would give an observed effect as described in the texts.
View user's profile View All Posts By User
DennyDevHE77
Hazard to Others
***




Posts: 168
Registered: 15-9-2014
Member Is Offline

Mood: No Mood

[*] posted on 25-7-2024 at 20:31


It wasn't about the stability of the jelly and its shelf life. When dynamite and other nitroglycerine explosives were in vogue, nitroglycerine was quite well purified, it was quite well stored for many years.

The question in this thread was about the severe drop in susceptibility after only a few days. More precisely, the question was what phenomenon causes this drop in susceptibility.

I guess it's my fault for wording it wrong. In post-Soviet countries, the degradation of jelly does not mean decomposition, but a drop in susceptibility. And that is what it is called in the specialized books.
View user's profile View All Posts By User
DennyDevHE77
Hazard to Others
***




Posts: 168
Registered: 15-9-2014
Member Is Offline

Mood: No Mood

[*] posted on 25-7-2024 at 20:52


I note that in the books where these experiments are actively described (that is, the books are just 30s), in all experiments detonator capsule number 8 was used. But it is not clear which one, then there was number 8 (1.6 g of mercury fulminate with 0.4 potassium chlorate) and the same number 8 (0.4 g mercury fulminate and 1.6 g tetryl)

[Edited on 26-7-2024 by DennyDevHE77]
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 920
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 29-7-2024 at 08:49


I think we understood your question well enough, and I stand by my answer: If the bubbles or other inhomogeneities disappear over time, the gel will become much less sensitive to high order initiation and may even require a booster (but low order detonation can still be achieved with weak detonators like inferior fulminate caps).
View user's profile View All Posts By User
Laboratory of Liptakov
International Hazard
*****




Posts: 1447
Registered: 2-9-2014
Location: Tel Aviv University
Member Is Offline

Mood: old jew

[*] posted on 29-7-2024 at 09:58


Tetryl has VoD max. 7300. Is it nothing extra VoD. And mercury fulminate 4250. Especialy FHg (in any amount in detonator) can cause low order detonation. But entire this thread is such theoretical ballancing around Maybe and what if.....:cool:



Development of primarily - secondary substances: CHP (2015) neutral CHP and Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024) Diper 60 (2025)
View user's profile View All Posts By User

  Go To Top