Author: Subject: Nitric acid storage
Chemgineer
Hazard to Others
***




Posts: 193
Registered: 25-5-2021
Member Is Offline


[*] posted on 21-4-2023 at 13:09
Nitric acid storage


I normally produce my nitric acid at 50% just due to the water content of my raw materials (magnesium nitrate and sodium bisulphate).

I know nitric acid is best stored in amber bottles but at 50% concentration would it be ok to store in clear glass?
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3621
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 21-4-2023 at 13:25


You can use glass for any concentration.
If clear (or amber) glass is used then protect from long exposures to sunlight,
I keep mine in the dark.

The problem is usually the cap and/or the cap liner.
PVC 'cling film' over the mouth of the bottle before screwing the cap on seems to be ok.

Edit.. regarding the reply below :
I was kindly donated some ptfe cap liners by a member here,
Good, but I need to find a suitable glue to keep them from occasionally falling out.
(maybe not the perfect diameter for my bottles)

[Edited on 21-4-2023 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Chemgineer
Hazard to Others
***




Posts: 193
Registered: 25-5-2021
Member Is Offline


[*] posted on 21-4-2023 at 13:26


What I normally do is cut a circular piece of 0.5mm PTFE sheet and line the inside of my caps.