Most promising primary battery chemsitry


Any ideas on the most practical battery chemistries to experiment with for highest energy densities possible. The battery can be primary… it’s almost better if it is. The best I can find is lithium thyionl chloride, however the discharge rates are about .1C, far too little.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3630
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 30-3-2022 at 00:37


silver is used as the anode of a primary cell that has high discharge rates,
with electrolyte added only when required, giving a very long shelf life.
mostly military applications.

A sodium anode in water should give a massive current - available as the sodium explodes.

Unless you want to spend years on battery research your best bet is to buy a commercial product.
Making a battery is reasonably easy, making a reliable battery is not.

[Edited on 30-3-2022 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
MineMan
National Hazard
****




Posts: 998
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 30-3-2022 at 03:47


Quote: Originally posted by Sulaiman  
silver is used as the anode of a primary cell that has high discharge rates,
with electrolyte added only when required, giving a very long shelf life.
mostly military applications.

A sodium anode in water should give a massive current - available as the sodium explodes.

Unless you want to spend years on battery research your best bet is to buy a commercial product.
Making a battery is reasonably easy, making a reliable battery is not.

[Edited on 30-3-2022 by Sulaiman]


Thank you for the reply. I see some papers where labs make a battery that has 1000wh/kg. I need storage capacity and medium discharge. It seems like producing them at scale is the challenge rather than making a few in the lab for testing?
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2723
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 30-3-2022 at 04:11


I think you're looking for Li-SVO (cathode: Ag2O*2V2O5), used for medical implants requiring the highest possible energy and power density:
https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3811938/

A fuel-air cell would have an even higher energy density, but low power output. And good luck "making" this, it's very, very hard.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
hodges
National Hazard
****




Posts: 525
Registered: 17-12-2003
Location: Midwest
Member Is Offline


smile.gif posted on 30-3-2022 at 15:19


I would be interested in seeing a lithium-fluorine fuel cell. A single cell should produce nearly 6 volts!

Sorry for being a "wise guy", but after examining the electromotive series I've always wondered if a cell made with the highest and lowest potential elements is feasible.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3630
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 30-3-2022 at 18:39


I suppose that anyone considering battery chemistry has had similar thoughts.

Due to geopolitics I guess that battery research is well funded at the moment.

My own brief attempts at diy batteries exposed how little electrochemistry I understand :)




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
MineMan
National Hazard
****




Posts: 998
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 31-3-2022 at 09:25


The Li SVO looks interesting… it’s still best by lithium thyional chlorides at 1400wh/kg… but these have low current discharge. It does seem challenging but reading some papers some chemistries are doable.

Lithium fluoride would be awesome. I wonder about lithium hydride and graphene fluoride!
View user's profile View All Posts By User