Author: Subject: Does anyone have experience with silicon wafers?
scienceboi
Harmless
*




Posts: 31
Registered: 12-9-2019
Location: California
Member Is Offline

Mood: Curious

[*] posted on 19-5-2021 at 18:28
Does anyone have experience with silicon wafers?


Since there is this whole global microchip shortage. I've begun researching how microchips are made, from sand to chip. However, a lot of information seems shallow and not truly informative. There are a lot of patents for tech so I'm guessing most of the processes are hidden behind proprietary walls. Are there any members who have worked with any part of the process? I'd love some advice on how to DIY some parts.

So far from researching the chip DIY scene, I found this guy. He's a good jumping off point but I'm still a bit lost




"Read not to contradict and confute; nor to believe and take for granted; nor to find talk and discourse; but to weigh and consider." -Francis Bacon
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1324
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 19-5-2021 at 20:37


So you want to invest half a million bucks into equipment to make your own chips?

The closest I've got is doing the schematic design for an LED driver. I had the benefit of good SPICE models for the 0.18um CMOS process we were using, supplied by the foundry.
I still have one of the engineering sample wafers on my shelf.

[Edited on 20-5-2021 by Twospoons]




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3692
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 19-5-2021 at 20:44


I had a tour of the Intel factory here...
ZERO chance of DIY!




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1716
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 19-5-2021 at 22:47


This is pretty much the limit for DIY semiconductors: https://en.wikipedia.org/wiki/Crystal_detector



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
scienceboi
Harmless
*




Posts: 31
Registered: 12-9-2019
Location: California
Member Is Offline

Mood: Curious

[*] posted on 19-5-2021 at 22:48


I'm naively convinced that there is a way to DIY, especially because of the guy I linked, Sam.

2nm process... that's never gonna happen. That scale really needs all the fancy equipment. But something on the micron level feels possible. That was back in the 70s. The price of tech already drops more or less tied to Moore's law. So the tech needed to make ICs should also generally drop in price as well. (or I gotta make it myself, oof)

However, that's on the making of the IC. What are your opinions on the silicon crystal/ingot manufacturing process? Would you say its more available to DIY?




"Read not to contradict and confute; nor to believe and take for granted; nor to find talk and discourse; but to weigh and consider." -Francis Bacon
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1716
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 20-5-2021 at 05:57


http://sam.zeloof.xyz (same person as OP links to).

Boy do I stand corrected. This is incredible work.




We're not banging rocks together here. We know how to put a man back together.