Author: Subject: Electroless plating Re on Mg
FragranceLover89
Hazard to Self
**




Posts: 72
Registered: 13-8-2019
Member Is Offline


[*] posted on 29-10-2020 at 16:05
Electroless plating Re on Mg


I attempted electroless deposition of Re on Mg to make a corrosion resistant Mg ring. I bought a sintered Re metal cylinder on ebay (XRD showed it matched Re) and put it in an ammonia/H2O2 solution to produce perrhenic acid. A gold colored iridescent film formed on the Mg after contact with the solution, which may have been a layer of Re. The ring later (4 months) oxidized in air and became rough. Adding vitamin c to the plating solution seemed to make an Re complex (red/orange color), however this did not effect plating on Mg. Mg and Re have similar crystal structures (hcp) and lattice constants. I don't know how safe Re is. Apparently tungsten and tungsten carbide are carcinogenic but Re seems more like manganese chemically so it might be safer?

I got the chance to melt some of the Re powder in a vacuum arc furnace and made a cool pellet (photo below).

* I just remembered I was inspired to do this after depositing a black (CuS) layer on Mg with copper/ammonia with some sulfide(?) while I was trying to de-tarnish silver. It was a really cool looking texture and surprisingly durable. If I remember correctly that solution was kind of a witches brew. It had borax, copper, gallium (very small amount), ammonia, magnesium, aluminum, and tarnished silver. The coating was really slick like boron but probably not boron. IDK.

IMG_0660.JPG - 1.5MB IMG_0661.JPG - 1.5MB

[Edited on 30-10-2020 by FragranceLover89]

[Edited on 30-10-2020 by FragranceLover89]

[Edited on 30-10-2020 by FragranceLover89]

[Edited on 30-10-2020 by FragranceLover89]

[Edited on 30-10-2020 by FragranceLover89]
View user's profile View All Posts By User
FragranceLover89
Hazard to Self
**




Posts: 72
Registered: 13-8-2019
Member Is Offline


[*] posted on 1-11-2020 at 19:57


Here is the rhenium coating ~1 year later. Note the golden yellow color.

IMG_0743.JPG - 458kBIMG_0744.JPG - 1.5MB
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7987
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 1-11-2020 at 23:56


I had a similar experience with zinc metal, added to an acidic solution of ammonium perrhenate. I added granules of very pure zinc to such a solution, hoping to get a nicely colored lower oxidation state compound in solution, but instead, the zinc became covered by a gold-colored (albeit much lighter than real gold) layer and the reaction quickly came to a standstill.

Rhenium metal does not have such a gold color. I have sintered rhenium pellets, 0.75 grams each, and these are grey. I also have a few square cm of rhenium foil. This has a silvery color. Maybe the mix of rhenium and the base metal on which the rhenium is plated has a more yellowish color?




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
chornedsnorkack
National Hazard
****




Posts: 539
Registered: 16-2-2012
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2020 at 06:53


Rhenium trioxide is also described as a red solid with a metallic lustre resembling copper, insoluble in water and dilute acids and bases.
View user's profile View All Posts By User
FragranceLover89
Hazard to Self
**




Posts: 72
Registered: 13-8-2019
Member Is Offline


[*] posted on 2-11-2020 at 18:42


I forgot to mention that this metal cylinder was originally clean white Mg. The dark spots also contain Rhenium. To get a lower oxidation state I would try adding vitamin C to perrhenates. I definitely saw a red/orange colored solution.

[Edited on 3-11-2020 by FragranceLover89]
View user's profile View All Posts By User
chornedsnorkack
National Hazard
****




Posts: 539
Registered: 16-2-2012
Member Is Offline

Mood: No Mood

[*] posted on 2-11-2020 at 21:52


Quote: Originally posted by FragranceLover89  
I forgot to mention that this metal cylinder was originally clean white Mg. The dark spots also contain Rhenium.


Rhenium dioxide is described as gray to black.
View user's profile View All Posts By User
FragranceLover89
Hazard to Self
**




Posts: 72
Registered: 13-8-2019
Member Is Offline


[*] posted on 3-11-2020 at 18:36


I am guessing you are right. It is likely a mixture of ReO2 and ReO3 in a super thin layer. It is iridescent so the gold color is likely due to thin film interference.