Extraction of silver from mixed silver salts
Hey everyone,
I have a bunch of silver salts from laboratory waste which consists of insoluble silver halides, oxides and metallic silver. I would like to purify
it and obtain silver ingots, preferably with as little wasted silver as possible.
What do you suggest I do? The problem is that I do not know the exact composition of the waste.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
You can boil the salts with NaOH to convert everything to silver oxide, then filter, wash and re-suspend. Now you can reduce the silver with dextrose
or sucrose to the metal.
|
|