finetune
Harmless
Posts: 14
Registered: 8-10-2019
Member Is Offline
|
|
Palladium recovery from 10% palladium on zinc carbonate and other question
A few weeks ago I bought 50g of 10% palladium on zinc carbonate on ebay for about 120eur. If the listing was true, I got 5g of palladium for less than
it´s current market value. What a great deal!
As I began to dissolve the the carbonate support with dilute acetic acid (appx 5-10%, p.a. grade GAA diluted without measuring) CO2 evolution was
evident. When the gas evoloution stopped, the residual foam was broken down with dH2O using a squirt bottle.
I wanted to wait for the Pd particles to settle but the particles seem to be so fine, even after two days+ it was impossible to shine trough using a
flashlight. My little black hole in a beaker. A solid layer on the bottom is evident though.
Filtering this suspension is impossible using normal filterpaper, I don´t even have to try. I have a Por4 fritted filter, maybe this one will do it,
but it is dirty as fuck, piranha didn´t eat the dirt and I am low on nitric atm.
Do you may have any good ideas?
And what was the catalyst used for? I never heard of zinc carbonate as support.
Finetune
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
Don't use a frit, you will never get it all out...
|
|
UC235
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
Filter it through a celite pad, wash with acid to remove zinc. Heat celite/Pd in aqua regia. Filter to collect PdCl4 solution. Boil down or
precipitate with ammonium chloride.
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Quote: Originally posted by finetune ![](images/xpblue/lastpost.gif) | A few weeks ago I bought 50g of 10% palladium on zinc carbonate on ebay for about 120eur. If the listing was true, I got 5g of palladium for less than
it´s current market value. What a great deal! | Mind if you post the link?
|
|
finetune
Harmless
Posts: 14
Registered: 8-10-2019
Member Is Offline
|
|
Using a frit will not be that much of a problem as I intend to work with aqua regia in the next step anyway.
Quote: Originally posted by UC235 ![](images/xpblue/lastpost.gif) | Filter it through a celite pad, wash with acid to remove zinc. Heat celite/Pd in aqua regia. Filter to collect PdCl4 solution. Boil down or
precipitate with ammonium chloride. |
Great! Thanks! I dont have any celite atm, but it is on my list anyway.
Quote: Originally posted by fusso ![](images/xpblue/lastpost.gif) | Quote: Originally posted by finetune ![](images/xpblue/lastpost.gif) | A few weeks ago I bought 50g of 10% palladium on zinc carbonate on ebay for about 120eur. If the listing was true, I got 5g of palladium for less than
it´s current market value. What a great deal! | Mind if you post the link? |
The link is not of any use anymore as I bought everything left. If you are interested I can sell you 5g in the original container for the price I got
it.
![DSC08215 (2).JPG - 1MB](http://www.sciencemadness.org/talk/files.php?pid=628435&aid=78552)
|
|