Synthesis of Hexaammine nickel II chloride


Hexaammine nickel II Chloride is a complex formed with nickel II Chloride and ammonia

Materials required

4g ammonium chloride
5g nickel II Chloride
Distilled water
10ml 30% ammonia

Procedure

Weigh out seperately 5g Nickel (II) chloride and 4g ammonium chloride in two seperate beakers.
Now preparing saturated solutions of them by
Adding 4ml of distilled water to nickel chloride and 10ml of water to ammonium chloride.
After preparation of the saturated solutions seperately, pour ammonium chloride solution into nickel chloride solution
Into this solution add 10ml of 30% cold ammonia and mix well. Allow the ppt to sediment now filter the precipitate. Wash the container with cold ammonia solution to get all the solid out into the filtration unit and also wash the solid in filter paper with cold ammonia .
Dry the precipitate and weigh.

Nickel ions in water forms a complex
With 6 molecules of H2O around nickel 2+ ion.
When we add ammonia this water molecules are replaced by 6 molecules of ammonia forming the complex
[Ni(H2O)6]2+(aq) + 6NH3(aq) ==> [Ni(NH3)6]2+ +6H2O
Thanks to everyone who helped me do this video

Here's the video to my version of synthesis
https://youtu.be/GUxen09r5C0

IMG_20191208_134803_222.jpg - 1.2MB





Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1242
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 8-12-2019 at 09:11


Nice synthesis :). What purpose have NH4Cl?
View user's profile View All Posts By User
UC235
National Hazard
****




Posts: 565
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 8-12-2019 at 10:10


Quote: Originally posted by Bedlasky  
Nice synthesis :). What purpose have NH4Cl?


Buffer. Otherwise, you get hexaammine nickel II hydroxide due to the high pH probably.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4355
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 8-12-2019 at 12:15


No, ammonium chloride is not needed. Perhaps it increases the chloride concentration so that you get a better yield.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 241
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 8-12-2019 at 16:13


Yes that's just to increase the chloride ions.common ion effect




Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4355
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 8-12-2019 at 16:50


You can also add methanol to help precipitate the complex.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
vibbzlab
Hazard to Others
***




Posts: 241
Registered: 6-11-2019
Member Is Offline

Mood: Always curious

[*] posted on 8-12-2019 at 22:42


I've got it all




Amateur chemist. Doctor by profession
Have a small cute home chemistry lab.


Please do check out my lab in YouTube link below

This is my YouTube channel
View user's profile Visit user's homepage View All Posts By User

  Go To Top