What is colloidal gold?
I would like to ask some questions regarding the uses of Colloidal Gold. Is it the same as colloidal silver? Can it be use as colloidal silver? Some
doctors say that it is used in making the drugs. Is it true? Should it also kept in liquid form as the colloidal silver? If you got any kinds
information about it, then please inform me.
[Edited on 12-2-2010 by Polverone]
|
|
Polverone
Now celebrating 21 years of madness
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline
Mood: Waiting for spring
|
|
This seems like quackery promotion with a side of spamming but since colloids are interesting I leave the thread open for now, having removed the
commercial link.
PGP Key and corresponding e-mail address
|
|
psychokinetic
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 558
Registered: 30-8-2009
Location: Nouveau Sheepelande.
Member Is Offline
Mood: Constantly missing equilibrium
|
|
Re: Drugs. It's a decent drug carrier. Don't know anything about manufacture.
I also recall one of my lecturers saying it can be used in some way to aid tumour detection.
“If Edison had a needle to find in a haystack, he would proceed at once with the diligence of the bee to examine straw after straw until he found
the object of his search.
I was a sorry witness of such doings, knowing that a little theory and calculation would have saved him ninety per cent of his labor.”
-Tesla
|
|
DDTea
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 940
Registered: 25-2-2003
Location: Freedomland
Member Is Offline
Mood: Degenerate
|
|
I know a professor who was seeking to functionalize colloidal gold particles with carbohydrate ligands. The logic was that these ligands would
specifically bind to certain receptors on cancerous cells. Once bound, these cancerous cells would incorporate the colloidal gold and be killed.
Cool idea. Of course, there were a host of complications with this idea (mostly that cancerous cells are quite unpredictable in their
structure/mechanisms of action) so it remains to be seen if this will have practical application!
"In the end the proud scientist or philosopher who cannot be bothered to make his thought accessible has no choice but to retire to the heights in
which dwell the Great Misunderstood and the Great Ignored, there to rail in Olympic superiority at the folly of mankind." - Reginald Kapp.
|
|
Freddybaby
Harmless
Posts: 4
Registered: 8-3-2011
Member Is Offline
Mood: No Mood
|
|
Here is a somewhat commercial link to making your own
http://www.ehow.com/how_5794704_make-colloidal-gold-home.htm...
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Purple of Cassius is said to be colloidal gold.
I've done it with HEPES (that made nanoparticles, pretty purple solution) and also with ascorbic acid (this gives you a larger particle that is red in
solution)
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "