[*] posted on 5-10-2010 at 08:38
How do you get high temperatures ?


For some processes (e.g. @Rogerywemaw's phosphorus furnace) you need high temperatures as for my sodium making and metal melting.
If you use high temp, how hot do you meed and how do you heat it ?
Do you have a furnace , propane / charcoal / wood/ electric arc ?
View user's profile View All Posts By User
psychokinetic
National Hazard
****




Posts: 558
Registered: 30-8-2009
Location: Nouveau Sheepelande.
Member Is Offline

Mood: Constantly missing equilibrium

[*] posted on 5-10-2010 at 11:35


Depends where exactly you need the heat.

If the entire environment needs to be hot, then a furnace is where it's at.




“If Edison had a needle to find in a haystack, he would proceed at once with the diligence of the bee to examine straw after straw until he found the object of his search.
I was a sorry witness of such doings, knowing that a little theory and calculation would have saved him ninety per cent of his labor.”
-Tesla
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 5-10-2010 at 21:02


Induction heater ;)



Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 5-10-2010 at 21:15


Tim, can you provide a rough cost estimate for materials for a homemade 2000w induction heater. I'm just curious.

I've seen one of those in action at a university foundry and they are impressive. It was powered by 440V, 3-phase, IIRC.




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 5-10-2010 at 21:16


Under $400, depending on where you find parts and how much is surplus (aka junk).

The 440V 3 phase ones go way up there. How would you like a 1600A circuit? :D Open a small steel mill with one that sized. :D :D

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
peach
Bon Vivant
*****




Posts: 1428
Registered: 14-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 6-10-2010 at 10:17


Induction won't be suitable for what he's doing. Neither will arcs.

Fire from wood or propane will work but basically you're after a resistive heating element. Like Silicon Carbide or Moly D if you want to roast the ass out of piece of quartz or stainless tube.

Nichrome, Kanthal and the other nickel / chrome wires are possibilities. And far cheaper to try out since you can pull the wire from a toaster.

Two many posts asking the same thing, note the splattering effect in the replies. :P

[Edited on 6-10-2010 by peach]