What happens when latex rubber reacts with oil?
It's commonly mentioned that latex rubber is attacked by oil, including skin oils. I was wondering, what is the specific chemistry that is going on
when this happens?
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
It simply dissoves!
No chemical reaction
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
DrP
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
I guess it depends on the level of cross linking in the rubber though. If highly cross-linked then rather than disolving it will soften as the oil
molecules work their way into the rubber structure. Old hard cracked rubber can be re-vitalised a bit by rubbing in some oil.