Phosphor for Hg vapour lamp


I have tried to find out the composition of the phosphor typically used for HG vapour lamps but have been unable. Anyone know it composition?



View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 1-9-2008 at 21:21


Generally a europium-doped yttrium vanadate-phosphate, calcium halophosphates doped with manganese and other elements, magnesium fluorogermanate, magnesium-aluminium oxides doped with several different elements, terbium/cerium doped lanthanum phosphate, and/or erbium doped yttrium oxide.


Let's see, some references:

http://www.geconsumerandindustrial.com/environmentalinfo/doc...

http://www.americanelements.com/ph.html#lo

http://www.baotou-rareearth.com/phosphor.html


http://www.sylvania.com/BusinessProducts/MaterialsandCompone...
in particular
http://www.sylvania.com/BusinessProducts/MaterialsandCompone...

http://www.phosphor-technology.com/products/products.htm