[*] posted on 18-1-2013 at 10:42


Sounds interesting, but remember that CaCl2 is soluble: A much better sodium derivative would be the carbonate/bicarbonate. The sulfate does not work for this process because, surprisingly enough, calcium sulfate has roughly the same solubility as the hydroxide.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 18-1-2013 at 21:30


I came up with an alternate idea to prepare NaOH from Fe, HCl, NH4OH and Na2CO3.

Step 1. Prepare Fe(OH)2 from, as an example, the reaction of NH4OH and FeCl2. The latter from:

Fe + 2 HCl --> FeCl2 + H2 (g)

Step 2. React Na2CO3 with Fe(OH)2:

Na2CO3 + Fe(OH)2 --> FeCO3 (s) + 2 NaOH

where on this last reaction, one needs an increased solubility of Ferrous hydroxide in Na2CO3 to move this reaction to the right. However, more likely the solubility is reduced with increasing OH- concentration and starting with an excess of Sodium carbonate may not be sufficient.

Perhaps better cheaper/available amphoteric alternatives from Al(OH)3, Cu(OH)2, Zn(OH)2 or Pb(OH)2. For example (see http://gcsechemistryhelp.tumblr.com/post/33791502799/in-my-c... ):

3 Na2CO3 + 2 Al(OH)3 —> 6 NaOH + Al2(CO3)3

Now, the particular issue with this synthesis is the unstable nature of Aluminum carbonate decomposing at 120 C into Al(OH)3 and CO2 in the presence of water. As both of these decomposition products could react with the newly formed NaOH, this could present a challenge (requires a low temperature synthesis). In general even without the decomposition of the Aluminum carbonate, any unreacted Al(OH)3 (need some excess Na2CO3) could be attacked by the newly created NaOH forming NaAl(OH)4 reducing NaOH yield.


[Edited on 19-1-2013 by AJKOER]
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 19-1-2013 at 11:27


Use the hypochlorite to make ferrate...
An old process (Loewig, DE 1650, 1877) for NaOH production not involving lime uses ferric oxide from iron ore. It is heated with sodium carbonate to form sodium ferrate. Apparently this can be washed with cold water and not be decomposed, removing excess carbonate. The addition of boiling water gives strong NaOH solution and Fe2O3 again, which can be reused. This solution is much stronger than that which can be produced by lime, without evaporation.




"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
chemicalmixer
Harmless
*




Posts: 17
Registered: 19-3-2012
Location: north america
Member Is Offline

Mood: friction sensitive

[*] posted on 19-1-2013 at 12:51


I think I have a better method to make lye, starting with baking soda:

First, heat the soda to convert it to washing soda:

2NaHCO3 --> Na2CO3 + H2O + CO2

Now, make a saturated solution of washing soda in DH2O, and make an electrochemical cell with it, by applying DC electricity to the solution using two nickel, or nickel-plated electrodes.

Nickel(III) oxide-hydroxide is not amphoteric, and thus not soluble in caustic solutions. This is why nickel iron batteries work (which use concentrated KOH as an electrolyte). Ni(III) oxide-hydroxide also conducts current much better than other similar metal oxides. An iron cathode would also work instead of Ni, but Ni must be used as the anode. Also, nickel is one of the easier metals that can be successfully plated by the home experimenter using common chemicals, thus an iron substrate could be heavily plated with nickel prior to use as an anode here.

A permeable partition could be used to keep the CO/CO2 formed at the anode from reacting with the sodium ions, but this is probably unnecessary. A pH meter could help determine when all of the carbonate has been converted to hydroxide.

[Edited on 19-1-2013 by chemicalmixer]
View user's profile View All Posts By User
Manifest
Script Kiddie Asshole
***




Posts: 229
Registered: 7-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 19-1-2013 at 15:03


Quote: Originally posted by chemicalmixer  
I think I have a better method to make lye, starting with baking soda:

First, heat the soda to convert it to washing soda:

2NaHCO3 --> Na2CO3 + H2O + CO2

Now, make a saturated solution of washing soda in DH2O, and make an electrochemical cell with it, by applying DC electricity to the solution using two nickel, or nickel-plated electrodes.

Nickel(III) oxide-hydroxide is not amphoteric, and thus not soluble in caustic solutions. This is why nickel iron batteries work (which use concentrated KOH as an electrolyte). Ni(III) oxide-hydroxide also conducts current much better than other similar metal oxides. An iron cathode would also work instead of Ni, but Ni must be used as the anode. Also, nickel is one of the easier metals that can be successfully plated by the home experimenter using common chemicals, thus an iron substrate could be heavily plated with nickel prior to use as an anode here.

A permeable partition could be used to keep the CO/CO2 formed at the anode from reacting with the sodium ions, but this is probably unnecessary. A pH meter could help determine when all of the carbonate has been converted to hydroxide.

[Edited on 19-1-2013 by chemicalmixer]


If he doesn't have Sodium Hydroxide, I highly doubt that he has DH2O
View user's profile Visit user's homepage View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 19-1-2013 at 15:18


Quote: Originally posted by S.C. Wack  
Use the hypochlorite to make ferrate...
An old process (Loewig, DE 1650, 1877) for NaOH production not involving lime uses ferric oxide from iron ore. It is heated with sodium carbonate to form sodium ferrate. Apparently this can be washed with cold water and not be decomposed, removing excess carbonate. The addition of boiling water gives strong NaOH solution and Fe2O3 again, which can be reused. This solution is much stronger than that which can be produced by lime, without evaporation.


Hmm. Ferrate(III), aka ferrite. Just to be clear! :)

Chrome might also be a candidate, though Na2Cr2O3 itself may be too soluble (and also lead to chromate!).

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 19-1-2013 at 15:53


Quote: Originally posted by 12AX7  
Hmm. Ferrate(III), aka ferrite. Just to be clear! :)


Your interjection is not clear. I'm obviously talking about +6 ferrate as it's always been known. My post was not a commentary on the patent and the ease of (or lack of) oxidation in that way.

...whether they are making Na2Fe2O4 or what, I wasn't recommending going that way...just mentioning it since hypochlorite came up...

[Edited on 20-1-2013 by S.C. Wack]




"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 19-1-2013 at 17:28


Quote: Originally posted by S.C. Wack  
Use the hypochlorite to make ferrate...
An old process (Loewig, DE 1650, 1877) for NaOH production not involving lime uses ferric oxide from iron ore. It is heated with sodium carbonate to form sodium ferrate. Apparently this can be washed with cold water and not be decomposed, removing excess carbonate. The addition of boiling water gives strong NaOH solution and Fe2O3 again, which can be reused. This solution is much stronger than that which can be produced by lime, without evaporation.


Here is a reference that confirms the above Fe2O3 and Na2CO3 fusion reaction producing a ferrite ion described as:

Na2C03 + Fe203 → 2NaFe02 + C02

Link: http://www.sumobrain.com/patents/wipo/Apparatus-method-produ...

The reaction apparently occurs at 'bright red heat' in a rotating furnace (see http://www.lenntech.com/chemistry/caustic-soda.htm ).

The hydrolysis reaction is probably given by:

NaFeO2 + 2 H2O = Fe(OH)3 + NaOH

The water is hot steam at 900 C and the Fe(OH)3 also breaks down releasing Fe2O3.

This fusion synthesis may not be practical for the home.
---------------------------------------------------------------------------------

I have, however, have been looking at wet room temperature ferrate production via FeCl3 and Na2CO3.H2O2 (Sodium percarbonate) plus a weak hydroxide. The Na2CO3. H2O2 is substitute candidate for NaClO + a strong base which are ingredients in the classic hypochlorite ferrate synthesis.


[Edited on 20-1-2013 by AJKOER]
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 20-1-2013 at 04:39


Quote: Originally posted by AJKOKER  

I have, however, have been looking at wet room temperature ferrate production via FeCl3 and Na2CO3.H2O2 (Sodium percarbonate) plus a weak hydroxide. The Na2CO3. H2O2 is substitute candidate for NaClO + a strong base which are ingredients in the classic hypochlorite ferrate synthesis.


[Edited on 20-1-2013 by AJKOER]


You know, ferrates are so unstable species that they only exist in very basic solutions, easily decompose to ferric oxides and stuff like that. So if you want to attempt synthesis of some oxidant, you would do better with wet synthesis of permanganate. Unfortunatelly, as it's been said already on this forum, yields are very small.

Ferrates are best synthesized using dry fusion method as I heard, maybe use molten NaOH and oxidant such as nitrate, chlorate? But yeah, then again you would be better using MnO2.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 20-1-2013 at 08:06


That's what I thought -- ferrate(VI) is so difficult to create, and so unstable, that it can't possibly be formed at high temperature from such simple reagents as soda ash and oxygen.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 21-1-2013 at 18:12


OK, per this reference ( http://www.lenntech.com/chemistry/caustic-soda.htm ), here is an old process for making NaOH. To quote:

"To make very strong caustic, zinc oxide is often used to remove the sulphide from the tank liquors : -

Na2S+ ZnO + H20 = 2NaOH + ZnS

The precipitated zinc sulphide is settled out, before evaporating the caustic liquor. By calcining the zinc sulphide, the zinc is reconverted to oxide."

Note, water is consumed in the above reaction permitting the formation of concentrated Sodium hydroxide.
---------------------------------------------

So to create the NaOH, one apparently needs Sodium sulfide and Zinc oxide. But, how does one make Na2S at home? Here is one possible route starting with Sulfur:

2 Al + 3 S --> Al2S3

Then add the Aluminum sulfide to an aqueous solution of Na2CO3. Expected reactions:

Al2S3 + 6 H2O --> 2 Al(OH)3 + 3 H2S

Na2CO3 + H2S --> NaHS + NaHCO3 (see http://books.google.com/books?id=rpzrIZW-OcEC&pg=PA387&a... )

Followed by boiling or aeration to oxidize the Sodium hydrogen sulfide (see www.allreactions.com/index.php/group-1a/natrium/sodium-hydro... ):

2 NaHS (solution) --> Na2S + H2S↑ (boiling)

[Caution: Hydrogen sulfide is quite a toxic gas. Upon deadening ones' sense of smell, it is also an insidious poison with a delayed mortality effect. Use ventilation and appropriate safety measures]

2n NaHS (solid) + (n - 1)O2 = 2 H2O + (2n - 4) NaOH + 2 Na2(Sn) [100—250° С]

Attention should be paid to avoid the presence of any unreacted H2S or Sulfur which could react with any created NaOH (forming NaHS, Na2S and/or Na2S2O3). The presence of polysulfides themselves may not present a significant issue (forming an insoluble Zinc polysulfide).

Lastly, a reference on Zinc oxide creation (link: http://www.imm.ac.cn/journal/ccl/1506/150630-733-03-0359-p4.... ). To quote:

"The simple approach (precipitation—heat treatment) to fabrication of ZnO prickly spheres by
dehydration of the precursor obtained via chemical reaction between Zn(CH3COO)2·2H2O
and NH3·H2O in the presence of surfactant (SDS) was reported. Compared with other
methods the reaction condition was considerably moderate and the temperature was lower.
Moreover, prickly spheres could be obtained in high yield."


[Edited on 22-1-2013 by AJKOER]
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 22-1-2013 at 09:45


Quote: Originally posted by Manifest  


If he doesn't have Sodium Hydroxide, I highly doubt that he has DH2O


Distilled water? I can get that from the local Safeway for 99 cents. I hope you aren't thinking of deuterium oxide...




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
chemicalmixer
Harmless
*




Posts: 17
Registered: 19-3-2012
Location: north america
Member Is Offline

Mood: friction sensitive

[*] posted on 22-1-2013 at 15:06


Quote: Originally posted by Manifest  
If he doesn't have Sodium Hydroxide, I highly doubt that he has DH2O


Distilled water would ideal, but not necessary. How about actually contemplating what I've said, instead of nitpicking with your BS, non-relavent criticism? Electrolysis of a Na2CO3 or NaHCO3 solution with a Ni anode seems a hell of a lot more pratical for the average home experimenter than building a lime kiln or making sodium ferrate.
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2013 at 05:21


Quote: Originally posted by AJKOER  
OK, per this reference ( http://www.lenntech.com/chemistry/caustic-soda.htm ), here is an old process for making NaOH. To quote:

"To make very strong caustic, zinc oxide is often used to remove the sulphide from the tank liquors : -

Na2S+ ZnO + H20 = 2NaOH + ZnS

The precipitated zinc sulphide is settled out, before evaporating the caustic liquor. By calcining the zinc sulphide, the zinc is reconverted to oxide."

Note, water is consumed in the above reaction permitting the formation of concentrated Sodium hydroxide.


Actually, per this reaction (see http://www.allreactions.com/index.php/group-1a/natrium/sodiu... ):

2 NaOH (conc. 60%) + H2O + ZnO = Na2[Zn(OH)4] (90°С )

one should be mindful of the reaction temperature (keep below 90 C) and/or the NaOH concentration (under 60%) in the presence of any excess ZnO per the synthesis:

Na2S + ZnO + H20 --> 2NaOH + ZnS (s)
View user's profile View All Posts By User
LanthanumK
Hazard to Others
***




Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline

Mood: No Mood

[*] posted on 23-1-2013 at 10:01


I tried the electrolysis method and after quite a lot of current only came up with a little NaOH. It is not the most efficient method but it does work.



hibernating...
View user's profile Visit user's homepage View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 23-1-2013 at 10:04


Depends on how long, how much current in amps, and what kind of cell you used. I assume the electrolysis of Na2CO3/NaHCO3 works because the carbon dioxide produced leaves the solution, thus shifting the reaction in favor of NaOH. This should work even in a 1-cell, concentrated apparatus, so I'll give this a shot when I get the time (and when I can find my darn nickel scraps!)
Titration of your NaOH, or boiling it down, weighing it, and comparing it to the starting Na salt (assuming the NaOH is now pure) would be a good method of determining efficiency.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
Manifest
Script Kiddie Asshole
***




Posts: 229
Registered: 7-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 25-1-2013 at 03:25


Quote: Originally posted by elementcollector1  
Quote: Originally posted by Manifest  


If he doesn't have Sodium Hydroxide, I highly doubt that he has DH2O


Distilled water? I can get that from the local Safeway for 99 cents. I hope you aren't thinking of deuterium oxide...


LOL. Sorry, it was late at night when I posted that....:P
View user's profile Visit user's homepage View All Posts By User
Manifest
Script Kiddie Asshole
***




Posts: 229
Registered: 7-12-2012
Member Is Offline

Mood: No Mood

[*] posted on 25-1-2013 at 03:35


Quote: Originally posted by chemicalmixer  
Quote: Originally posted by Manifest  
If he doesn't have Sodium Hydroxide, I highly doubt that he has DH2O


Distilled water would ideal, but not necessary. How about actually contemplating what I've said, instead of nitpicking with your BS, non-relavent criticism? Electrolysis of a Na2CO3 or NaHCO3 solution with a Ni anode seems a hell of a lot more pratical for the average home experimenter than building a lime kiln or making sodium ferrate.

I'm sorry. Again, it was late at night....
View user's profile Visit user's homepage View All Posts By User
science_guy1
Harmless
*




Posts: 2
Registered: 4-4-2013
Member Is Offline

Mood: No Mood

[*] posted on 4-4-2013 at 13:08


I read that sodium carbonate decomposes to sodium oxide at high temperatures.1 The sodium oxide could then be reacted with water to produce lye.

I propane torched a crucible containing 30g of sodium carbonate for ten minutes but I failed to produce sodium oxide. Perhaps a furnace would work.

Any thoughts on this method? I have not seen it discussed.

Also I saw a youtube video of someone electrolyzing molten NaCl and producing sodium metal. You could then throw the sodium metal in water to make lye.

Footnotes:
1: "In practice, ordinary glass is formed by melting sand (quartz crystals) with sodium carbonate and calcium carbonate. The carbonates decompose to the oxides plus carbon dioxide." - General Chemistry 9th ed, D. Ebbing

[Edited on 4-4-2013 by science_guy1]

[Edited on 4-4-2013 by science_guy1]

[Edited on 4-4-2013 by science_guy1]

[Edited on 5-4-2013 by science_guy1]
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 4-4-2013 at 14:43


Oh, for science's sake...
You're going to need a temperature much higher than what a propane torch can provide.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 9-4-2013 at 18:51


Here is a theoretically interesting preparation for NaOH with practical issues as it involves working with Chloramine (toxic and potentially explosive vapor, see MSDS at http://www.guidechem.com/dictionary/10599-90-3.html ).

NH3 (g) + NaOCl ---> NaOH + NH2Cl (g) (see http://www.buzzle.com/articles/mixing-bleach-and-ammonia.htm... )

More precisely, slowly pass ammonia gas (or, in the form of drops) into Sodium hypochlorite solution. Chloramine fumes should be liberated due to the exothermic reaction, leaving largely aqueous NaOH.

To address NH2Cl vapor, use a fumehood, or lead it into dilute H2O2. Reactions:

NH2Cl + H2O <--> HOCl + NH3

HOCl + H2O2 --> HCl + H2O + O2

However, using Chlorine bleach (NaOCl, NaCl, Na2CO3, NaOH,..see Chlorox product list at http://www.clorox.com/products/clorox-regular-bleach/ ), means that the NaOH product would be contaminated with salt and Sodium carbonate. Adding some NaOH to the final product solution and cooling should separate out the impurities as NaOH is about 3 and 8 times more soluble, respectively, than NaCl and Na2CO3.

Yet another issue with this reaction is that the Chloramine must be completely removed by warming from the solution. If not, some Hydrazine (described by Wikipedia as being 'highly toxic', see http://en.wikipedia.org/wiki/N2H4 ) can be formed:

NH2Cl + NH3 --> N2H4 + HCl

When the addition of NH3 to NaOCl is no longer reactive, adding more NaOCl to restart the process could also remove any formed Hydrazine (although this may prove to be unwise as the reaction between any formed N2H4 and NaOCl may prove to be too energetic even with a small addition of bleach, see the MSDS for pure Hydrazine at https://docs.google.com/viewer?a=v&q=cache:kHchCn9SNMkJ:... ).

Note, this preparation for Sodium hydroxide must be repeated several fold just to create a dilute impure solution of NaOH as the starting concentration of NaOCl (with NaCl and Na2CO3) is generally low, and given the exothermic nature of this reaction with toxic fume production (a significant safety issue), this dilution is actually desirable. Hence, this preparation is not a recommended practical path for several reasons, but I thought its associated issues should be properly addressed.

[EDIT] Chloramine has recently been incorporated in certain districts as a desirable water purification agent. I will not take sides on this issue here, but I believe, I have witnessed some down playing (white washing?) of the associated toxic and mutagenic properties of NH2Cl (as support, note the sparse MSDS by Guide Chemical cited above, which is one of the few remaining sample reports mentioning any negative issues). As such, readers should be conscious of this controversy when reading up Chloramine, and what I believe are valid toxicity issues, which are perhaps, IMHO, more recently not as properly put forward.


[Edited on 10-4-2013 by AJKOER]
View user's profile View All Posts By User
ElectroWin
Hazard to Others
***




Posts: 224
Registered: 5-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 17-6-2013 at 09:11


if your'e going to use NaHCO3 or Na2CO3, then you might as well skip all the sulphur and use lime to steal the carbonate:
Na2CO3 (aq) + Ca(OH)2 --> 2 NaOH (aq) + CaCO3 (s)

the CaCO3 is only slightly soluble. not sure what to do if you need much higher purity.
View user's profile View All Posts By User
annaandherdad
Hazard to Others
***




Posts: 391
Registered: 17-9-2011
Member Is Offline

Mood: No Mood

[*] posted on 18-6-2013 at 08:38


ktw_100, you're getting some great advice from these guys on how to make NaOH, and I'm all for doing something for its educational value. But NaOH is a cheap chemical, easily available from the hardware store as drain cleaner or from chemical supply places if you need purity. The amount of work involved in making it for yourself is hardly worth it, unless it's just for fun.



Any other SF Bay chemists?
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 18-6-2013 at 15:07


How concentrated NaOH solution can we get with baking soda reaction with lime?

I mean NaHCO3 will react with Ca(OH)2 to form CaCO3 and Na2CO3.

Na2CO3 will proceed to react with Ca(OH)2 to form CaCO3 and NaOH.

Once NaOH is formed, could we basically dissolve more Na2CO3 and Ca(OH)2 in already formed solution to obtain even higher concentrations?

What is the limit where NaOH could basically push solubility of other two reactants downwards?
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 19-6-2013 at 03:47


Quote: Originally posted by Random  
How concentrated NaOH solution can we get with baking soda reaction with lime?

I mean NaHCO3 will react with Ca(OH)2 to form CaCO3 and Na2CO3.

Na2CO3 will proceed to react with Ca(OH)2 to form CaCO3 and NaOH.

Once NaOH is formed, could we basically dissolve more Na2CO3 and Ca(OH)2 in already formed solution to obtain even higher concentrations?

What is the limit where NaOH could basically push solubility of other two reactants downwards?


Sodium bicarbonate isn't very soluble in water, so it's not a great choice.

With the slaked lime/washing soda method you can probably go to 30 % (or slightly higher) of NaOH. But isolating the NaOH as solid lye... that's the REAL challenge.

As others have surely remarked here: the slaked lime/soda (or potash) reaction is a nice little demonstration of a displacement reaction but lye is so cheap and so OTC (see soap making sites e.g.) that it's not worth trying to prepare at home in any significant quantities.