Seems to be a really old thread.
Why not use a PbO2 anode if making sulfuric acid?
One can easily make one from a bit of lead, check YT videos, there are examples many showing this procedure.
|
|
j_sum1
Administrator
Posts: 6326
Registered: 4-10-2014
Location: At home
Member Is Offline
Mood: Most of the ducks are in a row
|
|
Quote: Originally posted by Mateo_swe | Seems to be a really old thread.
Why not use a PbO2 anode if making sulfuric acid?
One can easily make one from a bit of lead, check YT videos, there are examples many showing this procedure. |
Or even easier. Use a lead anode. After a short amount of use it obtains a PbO2 coating. And then you have a nice PbO2 anode.
|
|