m1tanker78
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 685
Registered: 5-1-2011
Member Is Offline
Mood: No Mood
|
|
I had to think about that one for a second. Yeah, a chunk of sodium would be a dog treat from hell. ![:o](./images/smilies/shocked.gif)
Tank
Chemical CURIOSITY KILLED THE CATalyst.
|
|
RadioTrefoil
Harmless
Posts: 16
Registered: 11-7-2012
Location: New Zealand
Member Is Offline
Mood: Inert
|
|
Quote: Originally posted by vmelkon ![](images/xpblue/lastpost.gif) | Besides the chisle and kitchen knife advice above, you can heat sodium under oil until it melts and then you suck up the sodium with a glass syringe
and dump it into a mold of your choice.
There was a video of that on youtube. The guy had a 4.5 Kg brick. He had bought a glass syringe (large) for 5 $ from ebay. |
Haha, I saw that video (from SodiumInfo). It didn't look particularly safe, he just had a pan full of molten sodium on an open gas stove. Don't you
think it would be a bit of a fire hazard?
MESITYL FREAKING OXIDE
|
|
vmelkon
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline
Mood: autoerotic asphyxiation
|
|
To me, it looks like the part where he has the block in the pan is safe. The sodium is covered by oxide so it should be fine.
The part where he takes liquid sodium out looks dangerous. I have to admit I don't have experience with sodium. I don't know why it didn't immediately
oxidize (the part where the sodium was on top of the silicone molds). Weird.
|
|
Endimion17
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1468
Registered: 17-7-2011
Location: shores of a solar sea
Member Is Offline
Mood: speeding through time at the rate of 1 second per second
|
|
Quote: Originally posted by vmelkon ![](images/xpblue/lastpost.gif) | To me, it looks like the part where he has the block in the pan is safe. The sodium is covered by oxide so it should be fine.
The part where he takes liquid sodium out looks dangerous. I have to admit I don't have experience with sodium. I don't know why it didn't immediately
oxidize (the part where the sodium was on top of the silicone molds). Weird. |
It's never covered with oxide(s). The "rust" is a mix of hydroxide, carbonate and hydrogencarbonate. The older it is, the more hydrogencarbonate there
is.
What's protecting sodium is a thin layer of its protective liquid. It simply won't do any harm as long as it's wet with kerosene.
Sucking the melt with a syringe is not dangerous if the syringe can handle the temperature level. Even if the melt falls out, as long as it doesn't
contact incompatible compounds, it won't ignite. Sodium can ignite only when sodium vapors are present in quantities above mere traces, and that's
around its boiling point and above.
It might even be a good idea to leave it to solidify in a syringe. A nice ingot can be made that way.
|
|
Pages: