If any of you are looking for very good cell membranes for reductions or oxidations in a divided electrolytic cell, you can always use the plastic
membrane found inside virtually any lithium ion battery, I have used ones out of the pouch type li ion batteries for R/C hobby planes etc, they can be
applied with silicone adhesive to a plastic container with a section of it cut out, it adheres very well. Just do not let the cell temp rise above 50
Celsius, the micropores in the membrane start to close and their conductivity decreases.
|
|