[*] posted on 1-1-2009 at 23:12


The front layer is conductive SnO2, and I believe plays no PV other than being a transparent conductor. The back layer does play an active part in the PV process, and must be carbon or platinum on SnO2. In both cases the doping of the ITO or SnO2:F layer is to get to conduct.

Note that the TiO2 is not just ceramics grade stuff, but Degussa P25 nano-particle material which has a high anatase phase content, or be formed in place from a titanium alkoxide.

Some info on it here:

http://www.tkk.fi/Units/AES/studies/dis/halme.pdf

http://www.sardegnaricerche.it/documenti/13_143_200811201257...

http://infoscience.epfl.ch/record/101072

http://dssc.blog.sohu.com/62907297.html

http://www.solideas.com/solrcell/cellkit.html

http://ice.chem.wisc.edu/Catalog/SciKits.htm#Anchor-Nanocrys...
which includes a parts list and some suppliers.

another kit
http://www.alibaba.com/catalog/103792958/Dye_Sensitized_Sola...
View user's profile View All Posts By User
bquirky
Hazard to Others
***




Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline

Mood: No Mood

[*] posted on 2-1-2009 at 05:50


Hello,

Ive not attempted creating any kind of transparent conductive coating (i have enough trouble making any kind of coating conductive :) but are electrolytes completely out of the question for this kind of application ?

perhaps a very corse grid like current colector with the whole pannel immersed in an electrolyte that is non reactive with the PV cell ?

Just thinking outloud.
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 2-1-2009 at 07:33


It already has an electrolyte, a non-aqueous iodide-iodine containing one; where are you putting the second one? Water and O2 degrade the system, the anatase TiO2 is good at oxidising organics in the presence of O2 and light. Read the articles linked to at http://www.solideas.com/solrcell/coatglas.html#Articles

DSSC_diagram.jpg - 65kB
View user's profile View All Posts By User
bquirky
Hazard to Others
***




Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline

Mood: No Mood

[*] posted on 3-1-2009 at 02:07


ahh i see.
View user's profile View All Posts By User
ChrisWhewell
Hazard to Self
**




Posts: 66
Registered: 22-12-2009
Location: Austin
Member Is Offline

Mood: No Mood

[*] posted on 25-12-2009 at 07:53


http://www.teralab.co.uk/Experiments/Conductive_Glass/Conduc...