Blind Angel
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 845
Registered: 24-11-2002
Location: Québec
Member Is Offline
Mood: Meh!
|
|
Electroless Nickel Plating
[This topic seem suited for this forum since it's halfway trough electroplating]
Has anybody ever heard of electroless nickel plating? What is the composition of the solution? All I can find is that it's a Nickel/Phosphorous alloy,
but no in detail compostion of the solution. Anybody has any info/paper on that?
/}/_//|//) /-\\/|//¬/=/_
My PGP Key Fingerprint: D4EA A609 55E4 7ADD 8529 359D D6E2 33F6 4C76 78ED
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Here are a few references to assist you....solo
ftp://electrochem.cwru.edu/pub/estir/proc.txt
http://www.corrosion-doctors.org/MetalCoatings/Electroless.h...
http://electrochem.cwru.edu/estir/proc.htm#dtop
ftp://electrochem.cwru.edu/pub/estir/
[Edited on 10-6-2007 by solo]
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
Blind Angel
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 845
Registered: 24-11-2002
Location: Québec
Member Is Offline
Mood: Meh!
|
|
I gratefully thank you for the linké
Electroless nickel plating (From a Meeting of the American Society for Testing and Materials, ASTM Special Technical Publication No. 265)
ASTM, Philadelphia, PA 1959.
and
Electroless deposition of metals and alloys (From the 172nd Meeting of The Electrochemical Society, Honolulu, Oct. 1987, ECS Proceedings, Vol. 88-12)
M. Paunovic and I. Ohno (Ed), ECS, Pennington, NJ 1988.
would be interesting, the other are either redundant or only say: electroless is good for you, find somebody to do it.
/}/_//|//) /-\\/|//¬/=/_
My PGP Key Fingerprint: D4EA A609 55E4 7ADD 8529 359D D6E2 33F6 4C76 78ED
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
Composition of solution information........solo
http://www.alu-info.dk/HTML/alulib/modul/A00364.htm
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Be careful with the sodium hypophosphite. In many countries in the world this is a so-called list I chemical, and as such it is highly watched and
suspect. Sodium phosphite in fact is quite benign and not dangerous at all, but apparently it is an important precursor for meth-cooks and that's why
it is so suspect. This makes me mad .
|
|
Tacho
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 582
Registered: 5-12-2003
Member Is Offline
Mood: No Mood
|
|
This is a very comprehensive text on electroless nickel:
http://www.ias.ac.in/sadhana/Pdf2003JunAug/Pe1104.pdf
I once obtained some plating using magnesium hypophosphite instead of sodium hyphosphite.
Hope this helps.
|
|
Texium
|
Thread Moved 19-11-2023 at 11:58 |